CSA 70AT

Download data sheet

General Product Description

General Product Description The Canadian Standards Association (CSA) specification G40.20/G40.21 covers structural quality steel of a number of different product forms. SSAB produces structural quality plates and sheet in accordance with CSA G40.20/G40.21 with specified minimum yield strengths of 38 ksi to 70 ksi. CSA 70AT is a weldable, notch-tough steel with a specified minimum yield strength of 70 ksi for thicknesses up to 2.5 in. along with specified minimum Charpy V-notch impact toughness.

Dimension Range

Grade
Grade
70AT
Thickness
(in)
0.750 - 1.249
Width
(in)
72 - 120
Length
(in)
240 - 1176
Grade
Grade
70AT
Thickness
(in)
1.250 - 2.00
Width
(in)
72 - 120
Length
(in)
240 - 1104

 Width: Please inquire for plate widths less than 72 in. and inquire plate product over 120 in.

Length: Please inquire for plate lengths less than 240 in. and for lengths greater than the listed maxima. Plate length may be limited by maximum individual plate weight of 66,000 lbs. 

 

Mechanical Properties

Tensile testing is performed in the transverse direction. The required tensile properties are tabulated below:

Grade
Grade
70AT
Thickness
(in)
0.750 - 2.00
Yield strength 1)
(min ksi)
70
Tensile strength
(ksi)
85 - 115
Elongation in 2" 2)
(min %)
14
Elongation in 8" 2)
(min %)
12

1) Yield strength measured as 0.2% offset or 0.5% extension under load.

2) See elongation requirement adjustment of CSA G40.20-13 (Latest edition).

Impact Properties

Impact testing to be completed per CSA G40.21 requirements following Size Group requirements. Actual test temperature may be lower than standard temperature and will be reported with absorbed energy values.

Grade 1)
Grade 1)
70AT Category 1
Thickness
(in)
0.750 - 2.00
Minimum Longitudinal Average Absorbed Energy
(ft-lbs)
20
Test temperature
(°F)
32
Grade 1)
Grade 1)
70AT Category 2
Thickness
(in)
0.750 - 2.00
Minimum Longitudinal Average Absorbed Energy
(ft-lbs)
20
Test temperature
(°F)
0
Grade 1)
Grade 1)
70AT Category 3
Thickness
(in)
0.750 - 2.00
Minimum Longitudinal Average Absorbed Energy
(ft-lbs)
20
Test temperature
(°F)
-20
Grade 1)
Grade 1)
70AT Category 4
Thickness
(in)
0.750 - 2.00
Minimum Longitudinal Average Absorbed Energy
(ft-lbs)
20
Test temperature
(°F)
-50
Grade 1)
Grade 1)
70AT Category 5 2)
Thickness
(in)
0.750 - 2.00
Minimum Longitudinal Average Absorbed Energy
(ft-lbs)
—
Test temperature
(°F)
—

1) 70AT must be inquired to determine mandatory Charpy impact testing category and is subject to review before acceptance.