ASTM A514 Grade E

Download data sheet

General Product Description

ASTM A514 Grade E is a quenched and tempered alloy steel plate used in structural applications that require high yield strength combined with good formability and toughness. A514 Grade E has a minimum yield strength of 100 ksi up to 2.5 inches in thickness and 90 ksi for plates greater than 2.5 inches to 6 inches in thickness. Grade E may be ordered with supplemental Charpy V-notch toughness test requirements.

Applications

Typical applications for A514 Grade E include transport trailers, construction equipment, crane booms, mobile aerial work platforms, agriculture equipment, and heavy vehicle frames and chassis.

Available Dimensions

Grade
Grade
Grade E
Product type
Plate
Thickness
(in)
0.185 - 6.00
Width
(in)
60 - 131.9
Length
(in)
73 - 590

Mechanical Properties

Tensile Properties: Tensile testing is performed in the transverse direction according to ASTM A6 requirements. The tensile property and hardness requirements are tabulated below:

Grade
Grade
Grade E
Product type
Plate
Thickness
(in)
0.185 - 0.750
Yield strength
(min ksi)
100
Tensile strength
(ksi)
110 - 130
Elongation in 2"
(min %)
16
Reduction of area 1)
(min %)
35
Reduction of area 2)
(min %)
—
Hardness 3)
(HBW)
235 - 293
Grade
Grade
Grade E
Product type
Plate
Thickness
(in)
0.751 - 2.50
Yield strength
(min ksi)
100
Tensile strength
(ksi)
110 - 130
Elongation in 2"
(min %)
16
Reduction of area 1)
(min %)
35
Reduction of area 2)
(min %)
45
Hardness 3)
(HBW)
—
Grade
Grade
Grade E
Product type
Plate
Thickness
(in)
2.51 - 6.00
Yield strength
(min ksi)
90
Tensile strength
(ksi)
100 - 130
Elongation in 2"
(min %)
14
Reduction of area 1)
(min %)
—
Reduction of area 2)
(min %)
45
Hardness 3)
(HBW)
—

1) Reduction in area for 1.5 in. wide rectangular tension specimen.

2) Reduction in area for 0.5 in. round tension specimen.

3) For plates up to 0.375 in., a Brinell hardness test may be used instead of a tensile test for those plates not tensile tested in a 15 ton lot.