ASTM A1011 HSLAS Grade 50

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    Show specs in Imperial Metric

    General Product Description

    ASTM A1011 is a standard specification for hot-rolled, steel sheet and strip and coils of carbon steel, structural steel, high-strength low-alloy steel, high-strength low-alloy steel with improved formability, and ultra-high strength steel. The specification covers steel sheet, strip, and coils in thicknesses less than 0.230 in. A1011 High-Strength Low-Alloy Steel with Improved Formability (HSLAS-F) Grade 50 has a specified minimum yield strength of 50 ksi.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      HSLAS Grade 50 Class 1 Coils 0.188 - 0.2294.78 - 5.82 60 - 981500 - 2500
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness: Inquire for thicknesses <0.188 in. down to 0.079 in.

        Width: Inquire for widths <60 in. down to 39.4 in.

        Mechanical Properties

        Tensile testing is performed in the longitudinal direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Product type Thickness
          (inchesmm)
          Yield strength
          (min ksi)
          Tensile strength
          (min ksi)
          Elongation in 2"
          (min %)
          HSLAS Grade 50 Class 1 Coils 0.188 - 0.2294.78 - 5.82 50 65 22
          Compare parameters

          Select one parameter to compare

          Comparison

            Chemical Composition

            (Heat analysis, wt. %.)

            Hide/Show specific columns Edit
            Select columns to display
              Grade C
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Ti 1)
              (min %)
              V 1)
              (min %)
              Cb 1)
              (min %)
              Ni
              (max %)
              Mo
              (max %)
              Cu 2)
              (min %)
              Cr
              (max %)
              HSLAS Grade 50 Class 1 0.23 1.35 0.04 0.04 0.005 0.005 0.005 0.20 0.06 0.20 0.15
              Compare parameters

              Select one parameter to compare

              Comparison

                1) One or more of Cb, V, and Ti may be added. When added the min for that element applies, if not added then there is no minimum requirement.