    General Product Description

    ASTM A1011 is a standard specification for hot-rolled, steel sheet and strip and coils of carbon steel, structural steel, high-strength low-alloy steel, high-strength low-alloy steel with improved formability, and ultra-high strength steel. The specification covers steel sheet, strip, and coils in thicknesses less than 0.230 in. A1011 High-Strength Low-Alloy Steel with Improved Formability (HSLAS-F) Grade 70 has a specified minimum yield strength of 70 ksi.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (in)
      Width
      (in)
      HSLAS-F Grade 70 Coils 0.188 - 0.229 60 - 98
      Compare parameters

      Select one parameter to compare

      Comparison

        Inquire availability.

        Thickness: Inquire for thicknesses <0.188 in. down to 0.079 in.

        Width: Inquire for widths <60 in. down to 39.4 in.

        Mechanical Properties

        Tensile testing is performed in the longitudinal direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (in)
          Yield strength
          (min ksi)
          Tensile strength
          (min ksi)
          Elongation in 2"
          (min %)
          HSLAS-F Grade 70 0.188 - 0.229 70 80 20
          Compare parameters

          Select one parameter to compare

          Comparison

            Chemical Composition

            (Heat analysis, wt. %.)

            Hide/Show specific columns Edit
            Select columns to display
              Grade C
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Ti 1)
              (min %)
              V 1)
              (min %)
              Cb 1)
              (min %)
              Ni
              (max %)
              Mo
              (max %)
              Cu 2)
              (min %)
              Cr
              (max %)
              HSLAS-F Grade 70 0.15 1.65 0.020 0.025 0.005 0.005 0.005 0.20 0.16 0.20 0.15
              Compare parameters

              Select one parameter to compare

              Comparison

                1) One or more of Cb, V, and Ti may be added. When added the min for that element applies, if not added then there is no minimum requirement.