    ASTM A612 specification is the Standard Specification for Pressure Vessel Plates, Carbon Steel, High Strength, for Moderate and Lower Temperature Service. ASTM A612 encompasses carbon-manganese-silicon steel plates intended for use in welded pressure vessels for moderate and low temperature service.

    Dimension Range

    Hide/Show specific columns Edit
    Select columns to display
      Grade Thickness
      (in)
      Width
      (in)
      Length
      (in)
      A612 0.375 - 1.375 75 - 120 240 - 1020
      Compare parameters

      Select one parameter to compare

      Comparison

        Thickness: Inquire for thicknesses less than 0.375 in.

        Width: Inquire for widths less than 72 in. or greater than 120 in.

        Length: Maximum length for normalized plate is 600 in.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (in)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation in 2" 1)
          (min %)
          Elongation in 8" 1)
          (min %)
          A612 0.375 - 5.00 50 83 - 105 22 16
          A612 0.501 - 1.375 50 81 - 101 22 16
          Compare parameters

          Select one parameter to compare

          Comparison

            1) See specification A20 for elongation adjustment.