Název produktu | Rozměry | NORMY | Materiálový list |
|---|---|---|---|
| SSAB Domex 220LA | - | SSAB | |
| SSAB Domex 260LA | - | EN 10268 | |
| SSAB Domex 280LA | - | SSAB | |
| SSAB Domex 300LA | - | EN 10268 | |
| SSAB Domex 340LA | - | EN 10268 | |
| SSAB Domex 350LA | - | SSAB | |
| SSAB Domex 380LA | - | EN 10268 | |
| SSAB Domex 420LA | - | EN 10268 | |
| SSAB Domex 460LA | - | EN 10268 | |
| SSAB Domex 500LA | - | EN 10268 |
SSAB Domex 220LA
SSAB Domex 260LA
SSAB Domex 280LA
SSAB Domex 300LA
SSAB Domex 340LA
SSAB Domex 350LA
SSAB Domex 380LA
SSAB Domex 420LA
SSAB Domex 460LA
SSAB Domex 500LA