SSAB Domex® Tube 500MH

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

På denna sida

General Product Description

SSAB Domex Tube 500MH is extra-high-strength structural hollow section.

It is available in circular, rectangular, square and special shapes. Customized shapes and other tailoring options are available upon request. It is typically used in advanced engineering and construction where weight reduction, lower costs and safety are important. It meets the standard requirements of EN 10219 when applicable and is CE marked according to EN 1090-2.

SSAB Domex Tube 500MH is manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

Dimension Range

SSAB Domex Tube 500MH is available in circular, square and rectangular shapes.

Hide/Show specific columns Edit
Select columns to display
    Shapes Dimensions
    Circular (mmin) 42.4 - 323.91.67 - 12.75
    Square (mmin) 40x40 - 300x300
    Rectangular (mmin) 50x30 - 400x200
    Wall thickness (mmin) 2.0 - 12.50.079 - 0.492
    Mill length (mm) 6000 - 12 000/18 000 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Shapes
      Circular (mmin)
      Dimensions
      42.4 - 323.91.67 - 12.75
      Shapes
      Square (mmin)
      Dimensions
      40x40 - 300x300
      Shapes
      Rectangular (mmin)
      Dimensions
      50x30 - 400x200
      Shapes
      Wall thickness (mmin)
      Dimensions
      2.0 - 12.50.079 - 0.492
      Shapes
      Mill length (mm)
      Dimensions
      6000 - 12 000/18 000 mm

      Other shapes, sizes and lengths are available upon request.

      Circular Dimensions

      Hide/Show specific columns Edit
      Select columns to display
        Outer diameter (mmin) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
        42.41.67 1.99 2.19
        48.31.90 2.28 3.35 4.37
        60.32.37 2.88 4.24 5.55 6.82
        76.13.00 5.41 7.11
        88.93.50 6.36 8.38 10.4
        101.64.000 7.29 9.63 11.9
        1084.25 7.77 10.3 12.7
        114.34.500 8.23 10.9 13.5
        1275.00 9.17 12.1 15.0
        139.75.500 13.4 16.6 19.8 26.0 32.0
        168.36.626 16.2 20.1 24.0 31.6 39.0
        219.18.626 26.4 31.5 41.7 51.6
        27310.7 33.1 39.5 52.3 64.9 80.3
        323.912.75 47.0 62.3 77.4 96.0
        Compare parameters

        Select one parameter to compare

        Comparison

          Square Dimensions

          Hide/Show specific columns Edit
          Select columns to display
            Height x Width (mm) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
            40 x 40 2.31 3.30 4.20
            50 x 50 2.93 4.25 5.45
            60 x 60 3.56 5.19 6.71 8.13
            70 x 70 6.13 7.97 9.70
            80 x 80 7.07 9.22 11.3 13.2
            90 x 90 8.01 10.5 12.8 15.1
            100 x 100 8.96 11.7 14.4 17.0 21.4
            120 x 120 14.3 17.6 20.8 26.4
            140 x 140 16.8 20.7 24.5 31.4 38.1
            150 x 150 18.0 22.3 26.4 34.0 41.3
            160 x 160 23.8 28.3 36.5 44.4 52.6
            180 x 180 27.0 32.1 41.5 50.7 60.5
            200 x 200 30.1 35.8 46.5 57.0 68.3
            250 x 250 45.2 59.1 72.7 88.0
            300 x 300 54.7 71.6 88.4 108
            Compare parameters

            Select one parameter to compare

            Comparison

              Rectangular Dimensions

              Hide/Show specific columns Edit
              Select columns to display
                Height x Width (mm) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
                50 x 30 2.31 3.30 4.20
                60 x 40 2.93 4.25 5.45 6.56
                80 x 40 3.56 5.19 6.71 8.13
                80 x 60 6.13 7.97 9.70
                100 x 50 6.60 8.59 10.5
                100 x 60 7.07 9.22 11.3
                100 x 80 8.01 10.5 12.8
                120 x 60 8.01 10.5 12.8
                120 x 80 8.96 11.7 14.4
                140 x 80 13.0 16.0
                150 x 100 14.9 18.3 21.7 27.7
                160 x 80 14.3 17.6 20.8 26.4
                180 x 100 20.7 24.5 31.4 38.1
                200 x 100 22.3 26.4 34.0 41.3
                200 x 120 23.8 28.3 36.5 44.4 52.6
                250 x 100 26.18 31.11 40.23 49.11
                250 x 150 30.1 35.8 46.5 57.0 68.3
                300 x 200 45.2 59.1 72.7 88.0
                400 x 200 54.7 71.6 88.4 108
                Compare parameters

                Select one parameter to compare

                Comparison

                  Mechanical Properties

                  Hide/Show specific columns Edit
                  Select columns to display
                    Yield strength Rp0.2
                    (min MPa)
                    Tensile strength Rm
                    (MPa)
                    Elongation A5 1)
                    (min %)
                    Charpy-V -40°C 10x10 mm test specimen 2)
                    (J)
                    500 580 - 760 15 27
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Mechanical properties meet or exceed the requirements of EN 10219.

                      The mechanical properties for rectangular hollow sections are tested by SSAB on the longer side of the cross section.

                      1) The hollow sections with D/T < 15 (round) or (B + H)/2T < 12,5 (rectangular and square), the minimum value of elongation is reduced by 2.

                      2) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

                      Chemical Composition (ladle analysis)

                      Hide/Show specific columns Edit
                      Select columns to display
                        C
                        (max %)
                        Si
                        (max %)
                        Mn
                        (max %)
                        P
                        (max %)
                        S
                        (max %)
                        Nb
                        (max %)
                        V
                        (max %)
                        Ti
                        (max %)
                        0.16 0.25 1) 1.70 0.020 1) 0.012 1) 0.090 0.120 0.060
                        Compare parameters

                        Select one parameter to compare

                        Comparison

                          Chemical composition meets or exceeds the requirements of EN 10219.

                          The steel is aluminium-killed.

                          1) Value exceed the requirements of EN 10219.

                          Carbon Equivalent

                          Hide/Show specific columns Edit
                          Select columns to display
                            Wall Thickness (mm) 2.0 - 12.50.079 - 0.492
                            CEV (max %) 0.41
                            Compare parameters

                            Select one parameter to compare

                            Comparison

                              Wall Thickness (mm)
                              CEV (max %)
                              2.0 - 12.50.079 - 0.492
                              0.41

                              CEV value exceeds the requirements of EN 10219.

                              Tolerances

                              Tolerance Circular

                              Hide/Show specific columns Edit
                              Select columns to display
                                Characteristic Circular hollow sections
                                Tolerances meet or exceed the requirements of EN 10219
                                Outside diameter (D) (1 ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                                Out-of-roundness 2%, when D/T ≤ 100
                                Thickness (T) When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                                When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                                Straightness 0.20% of total length and 3 mm over any 1 m length
                                Mass per unit length Individual tube: ±6%
                                Mill length 0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                Exact length Agreed at the time of enquiry and order
                                Compare parameters

                                Select one parameter to compare

                                Comparison

                                  Characteristic
                                  Outside diameter (D) (1
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                                  Characteristic
                                  Out-of-roundness
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  2%, when D/T ≤ 100
                                  Characteristic
                                  Thickness (T)
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                  When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                                  When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                                  Characteristic
                                  Straightness
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  0.20% of total length and 3 mm over any 1 m length
                                  Characteristic
                                  Mass per unit length
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  Individual tube: ±6%
                                  Characteristic
                                  Mill length
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                  Characteristic
                                  Exact length
                                  Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  Agreed at the time of enquiry and order

                                  1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                  Tolerance Square

                                  Hide/Show specific columns Edit
                                  Select columns to display
                                    Characteristic Square hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    Outside dimensions (B, H) 1) When B, H < 100 mm ±1 % minimum ±0.5
                                    When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                    When B, H > 200 mm: ±0.6%
                                    Thickness (T) -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                    External corner profile When T ≤ 6 mm: 1.6 x T–2.4 x T
                                    When 6 mm < T ≤ 10 mm: 2.0 x T-3.0 x
                                    When T > 10 mm: 2.4 x T–3.6 x T
                                    Squareness of side 90° ±1°
                                    Concavity/convexity 0.8%, with a minimum of 0.5 mm
                                    Twist 2 mm + 0.5 mm/m
                                    Straightness 0.15% of total length and 3 mm over any 1 m length
                                    Mass per unit length Individual tube: ±6%
                                    Mill length 0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                    Exact length Agreed at the time of enquiry and order
                                    Compare parameters

                                    Select one parameter to compare

                                    Comparison

                                      Characteristic
                                      Outside dimensions (B, H) 1)
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      When B, H < 100 mm ±1 % minimum ±0.5
                                      When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                      When B, H > 200 mm: ±0.6%
                                      Characteristic
                                      Thickness (T)
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                      Characteristic
                                      External corner profile
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      When T ≤ 6 mm: 1.6 x T–2.4 x T
                                      When 6 mm < T ≤ 10 mm: 2.0 x T-3.0 x
                                      When T > 10 mm: 2.4 x T–3.6 x T
                                      Characteristic
                                      Squareness of side
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      90° ±1°
                                      Characteristic
                                      Concavity/convexity
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      0.8%, with a minimum of 0.5 mm
                                      Characteristic
                                      Twist
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      2 mm + 0.5 mm/m
                                      Characteristic
                                      Straightness
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      0.15% of total length and 3 mm over any 1 m length
                                      Characteristic
                                      Mass per unit length
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      Individual tube: ±6%
                                      Characteristic
                                      Mill length
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                      Characteristic
                                      Exact length
                                      Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      Agreed at the time of enquiry and order

                                      1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                      Tolerance Rectangular

                                      Hide/Show specific columns Edit
                                      Select columns to display
                                        Characteristic Rectangular hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        Outside dimensions (B, H) 1) When B, H < 100 mm ±1% minimum ±0.5
                                        When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                        When B, H > 200 mm: ±0.6%
                                        Thickness (T) -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                        External corner profile When T ≤ 6 mm: 1.6 x T–2.4 x T
                                        When 6 mm < t ≤ 10 mm: 2.0 x t-3.0x
                                        When T > 10 mm: 2.4 x T–3.6 x T
                                        Squareness of side 90° ±1°
                                        Concavity/convexity 0.8%, with a minimum of 0.5 mm
                                        Twist 2 mm + 0.5 mm/m
                                        Straightness 0.15% of total length and 3 mm over any 1 m length
                                        Mass per unit length Individual tube: ±6%
                                        Mill length 0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                        Exact length Agreed at the time of enquiry and order
                                        Compare parameters

                                        Select one parameter to compare

                                        Comparison

                                          Characteristic
                                          Outside dimensions (B, H) 1)
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          When B, H < 100 mm ±1% minimum ±0.5
                                          When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                          When B, H > 200 mm: ±0.6%
                                          Characteristic
                                          Thickness (T)
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                          Characteristic
                                          External corner profile
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          When T ≤ 6 mm: 1.6 x T–2.4 x T
                                          When 6 mm < t ≤ 10 mm: 2.0 x t-3.0x
                                          When T > 10 mm: 2.4 x T–3.6 x T
                                          Characteristic
                                          Squareness of side
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          90° ±1°
                                          Characteristic
                                          Concavity/convexity
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          0.8%, with a minimum of 0.5 mm
                                          Characteristic
                                          Twist
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          2 mm + 0.5 mm/m
                                          Characteristic
                                          Straightness
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          0.15% of total length and 3 mm over any 1 m length
                                          Characteristic
                                          Mass per unit length
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          Individual tube: ±6%
                                          Characteristic
                                          Mill length
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                                          Characteristic
                                          Exact length
                                          Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          Agreed at the time of enquiry and order

                                          1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                          Other hollow section products

                                          SSAB Domex® Tube 355J2H

                                          SSAB Domex® Tube 460MH

                                          SSAB Domex® Tube 550MH

                                          SSAB Domex® Tube Double Grade

                                          SSAB Weathering Tube 355WH

                                          SSAB Weathering Tube 500WH