How to weld > Welding consumables

Handling of consumables

In order to achieve the intended hydrogen content, it is important that the consumables are handled in accordance with their manufacturer.

Otherwise, the consumables can be subjected to excessive hydrogen pick-up from different substances in their environment.

General issues to consider in this respect are that:

  • The consumables are to be stored and kept away from contaminants. Examples of these are dampness, oil and grease.
  • Opened packages of consumables for MMA welding and fluxes for SAW often need to be stored at elevated temperatures. The reason is to avoid excessive hydrogen pick-up from the humidity in the air. This is normally done by keeping them in small furnaces especially designed for consumables. Unopened packages can normally be stored at room temperature.
  • Unopened and opened packages of solid wires and cored wires can normally be stored at room temperature. The cause is that they have a relatively high resistance for moisture pick-up.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 