SSAB Zero™ steel puts the circular economy into motion

SSAB is helping turn the idea of a circular economy into a working, real-world system – and a three-company team is at the heart of it. Together with The Greenbrier Companies and Alter Trading, SSAB followed recycled metals through the full life of steelmaking: from recycled steel in Iowa, into newly manufactured railcars, and back again to make new steel.

SSAB Americas partnered with The Greenbrier Companies and Alter Trading on a new circular steel project that followed recycled metals through the full life of steelmaking – from recycled metals to steel in Montpelier, Iowa, to use in newly manufactured railcars, and back again to bring recycled metals to steel production.

The project began in Iowa, where SSAB Zero™ steel was produced using recycled steel and fossil-free energy, resulting in near-zero fossil carbon emissions during production.

By rail to Greenbrier

From there, the coil was transported to SSAB’s cut-to-length facility in St. Paul, and then traveled by rail to Greenbrier, where it has been manufactured into 50 gondola railcars.

“This project demonstrates how near-zero emissions steel performs in real industrial applications. The circular economy only works if the material works at scale, under load, and within existing supply chains.”

Tom Cox, President of SSAB Americas

Closing the loop with Alter

In late summer, those railcars were delivered to Alter and are now in regular service, transporting recycled metals back to SSAB Iowa. The material they carry to SSAB is melted into new steel.

This collaboration relies on documented production processes, physical logistics, and material traceability – without the use of offsets.

Sharing the journey

SSAB, Greenbrier and Alter developed a joint social media and awareness campaign in 2026 to help tell this story. The campaign has now released the fourth of a planned four videos documenting key moments of the project, from steel production to fabrication and reuse. Leaders and team-members from all three companies celebrated the moment when a gondola railcar made from SSAB Zero™ arrived back at SSAB Iowa, filled with recycled metal ready to be made into new steel.

Thank you for visiting to learn more about this effort, and we hope you have enjoyed seeing how all three companies came together to help tell a circular economy story centered around low-emission steel.

About SSAB Zero™ steel

SSAB Zero™ is a commercially available steel made in Iowa, produced from recycled steel using fossil-free electricity and biogas, resulting in near-zero fossil carbon emissions during steel production. Fossil carbon emissions in SSAB’s production of SSAB Zero are less than 0.05 kg CO₂e per kg of steel in Scopes 1 and 2 under the Greenhouse Gas Protocol.

Read more about SSAB Zero™

Chapter 1: SSAB Zero™ steel in Iowa

The first chapter follows steelmaking at SSAB Iowa and the new steel heading to Greenbrier, with more to come across 2026.

Chapter 2: Gondola railcar production

The second chapter follows The Greenbrier Companies as they manufacture SSAB Zero™ steel into 50 new gondola railcars.

Chapter 3: Recycled metals return to SSAB Iowa

The third chapter follows Alter Trading as they use the new gondola railcars to carry recycled metals back to SSAB Iowa, closing the loop for new steel production.

Chapter 4: Successful recap

In our fourth and final chapter, leaders from all three companies look back at what this collaboration achieved together to lower emissions.

The next generation of recycled steel

SSAB Zero™ offers the same mechanical properties, performance, and quality as conventional SSAB steels, without relying on carbon offsets or mass-balance allocation.

Read about SSAB Zero™