Meeting vehicle weight limits, exceeding customer expectations

2 min read

A sleek semitrailer tipper body with the Hardox® In My Body sign of quality.

Country

Japan

Company

Takahashi Body

Industry

Trailers and body builders

Brand program

Hardox® In My Body

Higher payload plus tougher vehicle weight limits is an equation that doesn’t seem to add up. But with Hardox® 500 Tuf, Takahashi could lightweight its trailer bodies and take more payload.

No design changes, and easy to cut, bend and weld

Takahashi Body uses the same design as with its dumper bodies in Hardox® 450. The company had no production issues when switching to Hardox® 500 Tuf. Cutting, bending and welding could be performed with the same workshop equipment and techniques as for Hardox® 450.

Get technical advice
A white semi-trailer with body made in Hardox® 500 Tuf steel.

More upgrading, more recognition, more business

Takahashi Body plans to upgrade more of its dump trailer bodies and containers to Hardox® 500 Tuf. To improve the production process, the company is looking to invest in bending equipment capable of handling 12 m (39.4 ft.) long plates. This will reduce the need for welding and result in an even stronger product. 

“I feel that Hardox® 500 Tuf is a promising material for Japanese customers who need to follow stricter road regulations. With the higher hardness of Hardox® 500 Tuf, we can meet and even exceed our customers’ demands. Hardox® wear plate is a material that is highly recognized in Japan. And our membership in Hardox® In My Body really supports our reputation and sales. Customers can trust that we meet their expectations, which creates a very good relationship between us and our customers,”- Takahashi concludes.

Level up with Hardox® In My Body
Masataka Takahashi, sales director at Japanese Takahashi Body, proudly standing in front of a Hardox® In My Body certified tipper.
A strong yet lighweight green waste container made in Hardox® 500 Tuf steel.

When building the latest containers for transporting iron scrap, Takahashi Body replaced 6 mm (0.236”) Hardox® 450 with 5 mm (0.197”) Hardox® 500 Tuf. This reduction in thickness makes the steel plates used 17% lighter.

Takahashi

For more than 50 years, the Japanese company Takahashi Body has been designing and manufacturing truck bodies. Since 2000 it has been using Hardox® wear plate for its tipper bodies and containers. In 2010, the company became a qualified member of Hardox® In My Body, SSAB’s quality program for companies that use Hardox® wear plate in products that are designed and manufactured according to the strictest quality requirements.

Stay updated on Hardox® wear plate

A front wheel loader with bucket scraping up some Hardox® 500 Tuf.

All about Hardox® 500 Tuf in buckets

How to load more, save on maintenance and extend service life.

Here´s how
A hand holding the mobile app Hardox® Wearcalc, which calculates wear for different Hardox® steel grades.

Download the WearCalc App

Calculate how to increase payload and service life of your equipment using Hardox® wear plate

Try out the mobile app
Black and white logo of Hardox® In My Body on a dump body.

Hardox® In My Body - the sign of quality

A sign of quality and trust for the best products in the market.

Learn more about the sign of quality