SSAB Laminate FoodSafe

Download data sheet

General Product Description

SSAB Laminate FoodSafe from SSAB is available in white colors with a low gloss smooth surface, but can also be supplied with enhanced antistatic properties to minimize the contamination from airborne particles like dust. 

SSAB Laminate FoodSafe has typically a metal coated steel substrate with primer, adhesive and PVC-laminate on top side. Each layer is optimized for performance and processing benefits. 

SSAB Laminate FoodSafe offers excellent formability for a wide range of applications including walls, ceilings, doors in cold rooms and deep freezers, as well as refrigerated counters, institutional kitchens and production premises. 

SSAB Laminate FoodSafe is a highly durable and wear resistant laminated steel product that is resistant to chemicals and detergents which makes it easy to clean. It is non-toxic and suitable for direct contact with food and fully complies with current EU regulations (EU) No 10/2011, REACH regulations and is fully free of chromates.

The reverse side of the sheet is painted with a two-layer grey backside coating.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
11
Technical Properties
Technical Properties
Minimum inner bending radius
1 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
55 N
Technical Properties
Technical Properties
Highest operating temperature
60 °C
Technical Properties
Technical Properties
Lowest operating temperature
-40 °C
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
120 µm
Technical Properties
Technical Properties
Primer thickness, nominal
6 µm
Technical Properties
Technical Properties
Coating structure
Smooth
Technical Properties
Technical Properties
Steel designation 1)
S250GD-S350GD, DX51D
Technical Properties
Technical Properties
Zinc coating
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 1)
0.42 mm
Technical Properties
Technical Properties
Steel width 1)
1000 - 1400 mm

1) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

Colors

SSAB Laminate FoodSafe is available in white colors.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.