General Product Description

GreenCoat Pro BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating with Swedish rapeseed oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

GreenCoat Pro BT is highly durable and has mainly been developed for roofing applications like profiled roof tiles or standing seam systems. For tinsmith applications, GreenCoat PLX Pro BT and the FAP steel grade offered with GreenCoat Pro BT is additionally available. GreenCoat Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

GreenCoat Pro BT color coated steel is also optimized for wear resistance, weathering resistance and low resource consumption. It has greater durability than standard polyester products when exposed to people walking on the roof and other roof stresses. The product possesses excellent gloss retention and color fastness. It also provides good protection against corrosion reaching the RC5 class.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Pro BT complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Matt Regular
    Gloss 10 40
    Minimum inner bending radius 1.5 x sheet thickness 1.5 x sheet thickness
    Scratch resistance 35 N 35 N
    Lowest forming temperature -15 °C -15 °C
    UV radiation resistance RUV3 RUV3
    Corrosion resistance 1) RC5 RC5
    Stain resistance Very good Very good
    Highest operating temperature 100 °C 100 °C
    Fire classification, EN 13501-1 A2 s1 d0 A2 s1 d0
    Coating thickness, nominal (primer + top coat) 36 µm 36 µm
    Coating structure Structured Structured
    Steel designation 2) FAP, S280GD, S320GD, S350GD 3) FAP, S280GD, S320GD, S350GD 3)
    Zinc coating 275 g/m2 275 g/m2
    Min steel thickness 2) 0.50 mm 0.50 mm
    Steel width 2) 1000 - 1500 mm 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      3) FAP fulfills the requirements of EN 10346 DX52D.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

      34 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat Pro BT

      Nordic White

      RR1H3 / SS0020

      Regular, Matt

      Winter White

      RR20 / SS0005

      Regular

      Snow White

      RR19 / SS0001

      Regular, Matt

      Arctic White

      RR1L6 / SS0002

      Regular

      Polar White

      RR--- / SS6080

      Matt

      Powder White

      RR--- / SS0021

      Regular

      Limestone Grey

      RR268 / SS0022

      Regular, Matt

      Goosewing Grey

      RR2H5 / SS0461

      Regular

      Gravel Grey

      RR--- / SS0241

      Matt

      Quarry Grey

      RR287 / SS0244

      Regular, Matt

      Rock Grey

      RR237 / SS0061

      Regular

      Anthracite Grey

      RR2H8 / SS0087

      Regular, Matt

      Mountain Grey

      RR23 / SS0036

      Regular, Matt

      Ridge Grey

      RR2F7 / SS0035

      Regular

      Summit Grey

      RR--- / SS0454

      Regular

      Cliff Grey

      RR288 / SS0455

      Matt

      Nordic Night Black

      RR33 / SS0015

      Regular, Matt

      Walnut Brown

      RR32 / SS0387

      Regular, Matt

      Acorn Brown

      RR827 / SS0434

      Regular, Matt

      Coffee Brown

      RR820 / SS0384

      Regular, Matt

      Cottage Red

      RR29 / SS0758

      Regular, Matt

      Brick Red

      RR7F2 / SS0742

      Regular, Matt

      Fire Brick Red

      RR7G9 / SS0757

      Matt

      Harvest Yellow

      RR24 / SS0189

      Regular

      Silver Fir Green

      RR5J3 / SS0975

      Regular, Matt

      Leaf Green

      RR594 / SS0874

      Regular, Matt

      Pine Green

      RR11 / SS0830

      Regular

      Olive Leaf Green

      RR5H8 / SS6033

      Matt

      Lake Blue

      RR35 / SS0558

      Regular

      Metallic Silver

      RR40 / SS0045

      Regular, Matt

      Metallic Sterling

      RR974 / SS6045

      Matt

      Metallic Smokey Silver

      RR977 / SS6015

      Matt

      Metallic Dark Silver

      RR41 / SS0044

      Regular, Matt

      Metallic Copper

      RR979 / SS0778

      Regular

      Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.