SSAB’s toughest, ultra-hard protection plate.

Armox® Advance is SSAB’s toughest appliqué (add-on) protection plate for use where component weight reduction is essential. It is available in thicknesses between 4.0 and 7.9 mm, and not intended for further heat treatment.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Hardness
    (HRC)
    4.0 - 7.90.157 - 0.311 58 - 63
    Compare parameters

    Select one parameter to compare

    Comparison

      Thickness
      (mmin)
      4.0 - 7.90.157 - 0.311
      Hardness
      (HRC)
      58 - 63

       

      Mechanical Testing

      Rockwell hardness test EN ISO 6508-1. Each treatment individual.

      Ultrasonic testing

      According to EN 10160 Class E3S3.

      Chemical Composition (ladle analysis)

      Hide/Show specific columns Edit
      Select columns to display
        C *)
        (max %)
        Si *)
        (max %)
        Mn*)
        (max %)
        P
        (max %)
        S
        (max %)
        Cr*)
        (max %)
        Ni*)
        (max %)
        Mo*)
        (max %)
        B*)
        (max %)
        0.48 0.70 1.00 0.010 0.003 1.5 3.0 0.70 0.005
        Compare parameters

        Select one parameter to compare

        Comparison

          The steel is grain-refined. *) Intentional alloying elements.

          Tolerances

          More details are given in SSAB´s brochure Armox® Guarantees or on www.ssab.com.

          Thickness

          Hide/Show specific columns Edit
          Select columns to display
            Thickness
            (mmin)
            Tolerance
            (mmin)
            4.0 - 7.90.157 - 0.311 - 0.0 / + 0.6- 0.0 / + 0.0236
            Compare parameters

            Select one parameter to compare

            Comparison

              Thickness
              (mmin)
              4.0 - 7.90.157 - 0.311
              Tolerance
              (mmin)
              - 0.0 / + 0.6- 0.0 / + 0.0236

              Tolerances according to Armox® Thickness Guarantees.

              Armox® Guarantees meet the requirements of EN 10029 Class C, but offers narrower tolerances.

              Length and Width

              Tolerances conform to EN 10029 or to SSAB´s standard after agreement.

              Dimensional tolerances for plate with mill edge according to special agreement. 

              Shape

              Tolerances according to EN 10029.

              Flatness

              Flatness tolerance for thicknesses between 4.0 – 6.9 mm are according to Armox® flatness guarantee, which are more restrictive than EN 10029 Class N (steel type L). For thicknesses between 7.0 – 7.9 mm, the maximum accepted flatness deviation is 8 mm/m.

              Surface Properties

              According to EN 10163-2 Class B, Subclass 3.

              Delivery Conditions

              The delivery condition is Q (Quenched).

              Deliveryrequirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com