Hardox HiTemp wear plate improves service life at high temperatures

Hardox HiTemp is a welcome addition to SSAB’s Hardox wear plate family.

Hardox is a wear resistant steel with worldwide recognition. It improves productivity and extends service life in all kinds of industries since more than 40 years. During the years, Hardox has constantly evolved to reach new levels of hardness and toughness.

The new Hardox HiTemp meets an important wear challenge: Standing up to abrasive conditions in high heat environments.

Traditional quenched and tempered wear resistant steels experience a loss of hardness at higher temperatures, in the 300-500°C* range. 

 So far, alternative solutions for high temperature applications have been more costly and more complicated to work with.

Hardox HiTemp wear plate is a better answer. The high temperature performance of Hardox HiTemp is achieved by using high-quality raw material in combination with a carefully controlled manufacturing process. 

Hardox HiTemp can be cut, welded, machined and cold formed by the same kind of workshop machinery and technology as other Hardox grades and conventional steel.

All this adds up to making Hardox HiTemp an ideal choice for high temperature wear applications in many areas—particularly in process industries such as steel, cement and coal power plants, and recycling and asphalt industries.

*The temperature range is not strict and depends on the wear conditions. 300-500°C is equivalent to around 570-930°F.

For more information, please visit the Hardox HiTemp product page.

 

For more information on the performance of Hardox HiTemp, please contact:

Jenny Brandberg Hurtig Ph.D.

Product Manager Wear Plate, SSAB Special Steels

D +46 155 25 46 18   M +46 70 237 30 85

Email: [email protected]

 

 

附件

Related articles

其它新闻稿芬兰Ponsse公司推出的新一代林业收割机成功入围 2015 年“瑞典钢铁奖”(Swedish Steel Prize)最终提名
瑞典钢铁奖, 悍达, Strenx
其它新闻稿Milotek 开发的全新轨道运输系统入围 2015 年“瑞典钢铁奖”(Swedish Steel Prize)
瑞典钢铁奖, 悍达, Strenx
其它新闻稿Fácil System 生产的耐磨刀具荣获 2015 年“瑞典钢铁奖”最终提名
瑞典钢铁奖, 悍达