Strenx® 900 E/F
Download data sheet
Download data sheet
Upgrading from Strenx® 900 E/F to Strenx® 960 E/F means you can improve the performance and reduce the weight of your equipment. The increase in yield strength translates to a similar increase in the equipment’s load-bearing capacity. Get in touch with our steel specialists at SSAB Tech Support or SSAB Knowledge Service Center for an update on upgrading.