Thép hiệu suất Strenx
Thép hiệu suất Strenx

Strenx® 100

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page
Show specs in Metric Imperial

General Product Description

Strenx® 100 is a structural steel with a minimum yield strength of 690 Mpa. Strenx® 100 meets the requirements of ASTM A514, Grade S,

for thicknesses up to 63.50 mm.

Dimension Range

Strenx® 100 is supplied in plate thicknesses of 4.762 - 127.0 mm. More detailed information on dimensions is provided in the dimension program at www.ssab.com.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Yield strength Rp0.2
    (min MPaksi)
    Tensile strength Rm
    (MPaksi)
    Elongation A50 1)
    (min %)
    Reduction of area
    (min %)
    4.76 - 19.050.1875 - 0.7500 690100 760 - 890110 - 130 16 35
    19.06 - 63.500.7500 - 2.500 690100 760 - 890110 - 130 16 35 2)
    63.51 - 101.602.500 - 4 65094 700 - 890110 - 130 14 35 2)
    101.61 - 127.004 - 5 65094 700 - 890102 - 130 14 35 2)
    Compare parameters

    Select one parameter to compare

    Comparison

      1) For transverse test pieces according to ASTM A6 and A370.

      2) For 1-1/2” wide tension test samples. If 1/2” round samples are used, the minimum RA is 45%.

      Impact Properties

      Hide/Show specific columns Edit
      Select columns to display
        Product Min impact energy for transversal testing,
        Charpy V 0.393x0.393" test specimen 1)
        Strenx® 100 67 J / -40 °C50 ft-lbs / -40 °F
        Compare parameters

        Select one parameter to compare

        Comparison

          Product
          Strenx® 100
          Min impact energy for transversal testing,
          Charpy V 0.393x0.393" test specimen 1)
          67 J / -40 °C50 ft-lbs / -40 °F

          1) Average of three tests. Single value min 2/3 of specified average.

          For thicknesses between 6 - 11.9 mm, sub-size Charpy V-specimens are used. The specified minimum value is then proportrional to the cross-sectional area of the specimen compared to a full-size specimen (10x10 mm).

          Chemical Composition (ladle analysis)

          Hide/Show specific columns Edit
          Select columns to display
            C *)
            (max %)
            Si *)
            (max %)
            Mn*)
            (max %)
            P
            (max %)
            S
            (max %)
            Cr*)
            (max %)
            Ni*)
            (max %)
            Mo*)
            (max %)
            B*)
            (max %)
            0.20 0.60 1.60 0.020 0.010 0.80 2.0 0.70 0.005
            Compare parameters

            Select one parameter to compare

            Comparison

              The steel is grain refined. *) Intentional alloying elements.

              Carbon Equivalent CET(CEV)

              Hide/Show specific columns Edit
              Select columns to display
                Thickness
                (mmin)
                4.762 - 31.7500.1875 - 1.250 31.751 - 50.8001.250 - 2 50.801 - 101.6002 - 4 101.601 - 127.004 - 5
                Max CET(CEV) 0.32 (0.46) 0.36 (0.52) 0.39 (0.58) 0.41 (0.67)
                Compare parameters

                Select one parameter to compare

                Comparison

                  Tolerances

                  More details are given in SSAB’s brochure Strenx® Guarantees.

                  Thickness

                  Tolerances according to Strenx® Thickness Guarantees.
                  Strenx® Guarantees meets the requirements of EN 10029 Class A, but offers narrower tolerances.
                  EN 10029 meets and exceeds the requirements for ASTM A6.

                  Length and Width

                  Tolerances on length and width according to ASTM A6.

                  Shape

                  Tolerances according to ASTM A6.

                  Flatness

                  Tolerances on flatness according to Strenx® Flatness guarantee Class C, which are twice as good as the ASTM A6 flatness requirements. 

                  Surface Properties

                  According to ASTM A6.

                  Delivery Conditions

                  The delivery condition is Quenched and Tempered. The plates are delivered with sheared or thermally cut edges. Untrimmed edges after agreement.

                  Delivery requirements can be found in SSAB’s brochure Strenx® Guarantees.

                  Fabrication and Other Recommendations

                  Welding, bending and machining

                  Recommendations are found in SSAB’s brochures at www.ssab.com or consult Tech Support.

                  Workshop guidelines for Strenx® 100 refer to the same recommendations as for Strenx® 700. Bending guarantees according to Strenx® bending guarante class A.

                  Strenx® 100 has obtained its mechanical properties by quenching and subsequent tempering. The properties of the delivery condition cannot be retained after exposure to temperatures in excess of 580ºC.

                  Appropriate health and safety precautions must be taken when welding, cutting, grinding or otherwise working on this product. Grinding, especially of primer coated plates, may produce dust with a high particle concentration.