General Product Description

Docol PHS 1800 is cold rolled and alloyed with a small percentage of boron to improve hardenability. This steel is specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Standard Condition Test direction
    Typical yield strength Rp0.2
    (MPa)
    Typical tensile strength Rm (MPa) Typical elongation A80
    (%)
    Docol PHS FH 1800 SSAB Full Hard T 970 1070 4
    Docol PHS CR 1800 SSAB As delivered Annealed T 350 500 27
    SSAB Hot stamped 1) T 1300 1800 6
    Compare parameters

    Select one parameter to compare

    Comparison

      1) Properties depend on the process.

      Chemical Composition (ladle analysis)

      Hide/Show specific columns Edit
      Select columns to display
        C
        (%)
        Si
        (%)
        Mn
        (%)
        P
        (max %)
        S
        (max %)
        Cr
        (max %)
        B
        (%)
        0.27 - 0.33 0.15 - 0.35 1.00 - 1.45 0.025 0.010 0.35 0.0008 - 0.0050
        Compare parameters

        Select one parameter to compare

        Comparison

          Tolerances

          Cold rolled (UC): Tolerances in accordance to EN 10131.

          Customized dimensional and shape tolerances are available upon request.

          Surface Treatments

          Uncoated (UC): available as oiled.

          All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

          Fabrication and Other Recommendations

          For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

          Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

          Docol® PHS steel product offer

          Docol® PHS 1500 press hardening

          Docol® PHS 1800 press hardening

          Docol® PHS 2000 press hardening

          İlgili içerik