    General Product Description

    Docol PHS 1800 is cold rolled and alloyed with a small percentage of boron to improve hardenability. This steel is specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

    Dimension Range

    Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

    Slit strip and cut to length sheets are available upon request.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Standard Condition Test direction
      Typical yield strength Rp0.2
      (MPa)
      Typical tensile strength Rm (MPa) Typical elongation A80
      (%)
      Docol PHS FH 1800 SSAB Full Hard T 970 1070 4
      Docol PHS CR 1800 SSAB As delivered Annealed T 350 500 27
      SSAB Hot stamped 1) T 1300 1800 6
      Compare parameters

      Select one parameter to compare

      Comparison

        1) Properties depend on the process.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          C
          (%)
          Si
          (%)
          Mn
          (%)
          P
          (max %)
          S
          (max %)
          Cr
          (max %)
          B
          (%)
          0.27 - 0.33 0.15 - 0.35 1.00 - 1.45 0.025 0.010 0.35 0.0008 - 0.0050
          Compare parameters

          Select one parameter to compare

          Comparison

            Tolerances

            Cold rolled (UC): Tolerances in accordance to EN 10131.

            Customized dimensional and shape tolerances are available upon request.

            Surface Treatments

            Uncoated (UC): available as oiled.

            All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

            Fabrication and Other Recommendations

            For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

            Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

            Docol® PHS steel product offer

            Docol® PHS 1500 press hardening

            Docol® PHS 1800 press hardening

            Docol® PHS 2000 press hardening

            İlgili içerik