HDPE coated RD® piles for TYKS hospital, Finland

Successful project in tight time frame and demanding soil conditions

Läs mer

HDPE coated RD® piles for TYKS hospital, Finland

Successful project in tight time frame and demanding soil conditions

Our solution

Due to tight schedule of the project and demanding soil conditions, drilled RD piles were chosen for the project. Pile sizes RD800, RD600 and RD400 were used. RD800 piles are drilled three meters (4xD) and smaller ones 2 meters into the bedrock and grouted to the hole to ensure rigid connection. Piles are inclined and also tension anchors are used to take heavy accidental lateral and lifting loads.

In TYKS T3 project RD800 piles are exposed to de-icing salt and piles were protected against corrosion with 3-layer HDPE coating on piles. Additional to the coating, the resistance of the piles has been calculated with extra 2 mm corrosion allowance to wall thickness.

Customer case

Turku University Hospital (TYKS) is building a massive new building, named T3 Hospital, on top of existing E18 freeway and a rail road. New building will have total area of 54 000 m2 in eight stories. Total budget for the project is 158 M€.

Due to cold winters in Finland, a de-icing salt is often used for roads. This causes severe corrosion environment for steel piles.

“We prepared for damages in the coating with training of repair and a big bunch of repair materials. Now we have installed 97 pcs of coated piles and we have used only handful of repair patches. Our installation team has learned more gentle way to handle piles. I think this helps us also in normal projects, because they are handling also un-coated piles with more care.” Kai Jaakkola, Drilling supervisor, Lemminkäinen.

Delivery (2016):

  • RD220/12.5, RD400/10, RD400/12.5, RD600/14.2 in total 2 221 m, 269 pcs
  • HDPE coated piles: RD600/12.5, RD600/14.2, RD800/12.5 in total 2 175 m, 204 pcs

Co-operation partners:

  • Investor: Turku University Hospital (TYKS)
  • Contractor: Lemminkäinen
  • Design: Ramboll Finland Oy


RD® pile wall in Malmö hospital, Sweden

Minimum vibration, noise and disturbance to the surroundings

Läs mer

RD® pile wall in Malmö hospital, Sweden

Minimum vibration, noise and disturbance to the surroundings

Our solution

RD® pile wall has been chosen as a retaining wall solution for parts of the Malmö hospital investment project. RD pile wall was chosen as a solution due to minimum vibration as well as minimum noise and disturbance to the surroundings compared to other solutions.

Customer case

Region Skåne in Sweden is investing heavily on building a new future hospital in Malmö. Malmö hospital area investments include two new health care buildings, a new service center and an expanded culvert system. The work is expected to be completed by 2022.

Regular scheduled deliveries took place between June and October 2016. First part of the RD pile wall was built for new hospital building with two levels of basements. Second part of the RD pile wall was built for the culvert F. Next spring there will be a need for one more RD pile wall for another culvert.

Project is located in the city center of Malmö. Limited storage space required well scheduled deliveries.

Delivery (2016):

  • RM-RF interlocked RD320/12.5 piles in total close to 10 km, 665 pieces (1030 tons)

Co-operation partners:

  • Investor: Region Skåne (Responsible for healthcare and public transport, business development, culture, infrastructure, social planning and environmental and climate-related issues in Skåne)
  • Piling contractor: Skanska Sverige AB Grundläggning

SSAB median barriers to highway VT23, Finland

Fast and easy installation

Läs mer

SSAB median barriers to highway VT23, Finland

Fast and easy installation

Our solution

SSAB's median barrier is an effective way of improving traffic safety. Median barriers are used on roads between opposing lanes to prevent collisions between vehicles.

SSAB C210/130X4 has replaced the old model of median barrier, Box beam. The aim was to develop economical solution for customer. Number of components has been minimized to achieve cost efficient installation. There are no special screws with limited availability required. Also cost efficiency of the median barrier system has been improved by introducing high-strength steel grades.

Customer case

Highway VT23 is 517 km long from Pori to Joensuu. Kypäräjärvi passing line is situated 80 km before Joensuu.

Kuu Ras Oy installed SSAB C210/130X4 median barriers in September. This was the first installation of SSAB C210/130X4 median barriers for Kuu Ras Oy. According to them this median barrier is faster and easier to install than the previous model, Box beam. The connection is better and it includes fewer screws which makes it faster to install.

Delivery (2016):

  • SSAB C210/130X4 median barrier in total 1 860 m
  • SSAB side barrier in total 3 780 m

Co-operation partners:

  • Investor: Finnish Transport Agency
  • Installer: Kuu Ras Oy

RRs® piles in KSSHP’s major hospital project in Jyväskylä, Finland

Savings by replacing larger RR® piles with smaller size RRs® piles

Läs mer

RRs® piles in KSSHP’s major hospital project in Jyväskylä, Finland

Savings by replacing larger RR® piles with smaller size RRs® piles

Our solution

Original design of the project included significant amount of RR400/12.5 and RR320/12.5 piles. Those were replaced mostly by RRs220/10 due to material savings realized by stronger steel grade and better resistance-weight ratio. Alternative solution enabled also use of pile elements which resulted in time savings when splicing is easier and faster compared to splice welding. Also material waste is minimized when leftover piece can be utilized in next pile. Smaller diameter piles mean also less displacement and disturbance of soil in relation to the load-bearing capacity of the pile. Alternative solution resulted in 32% total cost savings. Cost savings in rock shoes was 64%. 

Customer case 

New hospital will be part of Central Finland Health Care District (KSSHP), which is the largest non-university hospital district in Finland. Hospital is built in Kukkumäki, Jyväskylä. Building project continues until 2020 and cost estimation is 398,5 m€.

Piling work is realized in two phases; 1st phase was done during Nov-Dec 2016 including 60% of the piling and 2nd phase is done during March-April 2017. Pile deliveries have been reliable and accurate. Piling has gone according to expectations and time schedule. Pile lengths corresponded quite accurately with the expectations based on soil investigation. Pile lengths have been 1.5-13.0 meters. Soil base is sandy and partly rocky, but it has not caused any problems like compaction.

“Pile deliveries have been able to be synchronized with the progress of the piling so that there have been no need for big intermediate storages at the job site.” Henri Laitila, Site manager, Kantolan Paalutus Oy

Delivery (2016-2017):

  • RRs220/10 totally 18 km, 2 113 pcs
  • RR170/10 totally 3.3 km, 380 pcs

Co-operation partners:

  • Investor: Central Finland Health Care District (KSSHP)
  • Main contractor: SRV Keski-Suomi
  • Piling contractor: Kantolan Paalutus Oy
  • Design: Ramboll Finland Oy

RR® piles in Akademiska Sjukhuset Uppsala, Sweden

Restrictions due to water catchment area and demanding deliveries

Läs mer

RR® piles in Akademiska Sjukhuset Uppsala, Sweden

Restrictions due to water catchment area and demanding deliveries

Our solution

SSAB’s extensive delivery included 34 km of RR220/10 pile elements.  SSAB answered the demand from it’s customer Hercules Grundläggning AB; supplying large amount of piles and accessories quickly by using special flat trucks.

Customer case

The project is included in investment for the University Hospital that will double the base by 50% in 7 years. Land contract was one of the largest in modern times in the county.

The challenge for the customer was that the project was in Uppsala water catchment area which led to restrictions on equipment and materials.

Limited space and high production rate meant many machine units that occasionally prevented the other. This also put great demands on the exact material supplies.

The project expanded by about 40% when the average length was 17 m instead of the tendered 12 m.

Client’s demand included dimensioning of piles to manage load capacity of 1550 kN and dimensioning of sheet piles for excavation depths between 5-14 m. Sheet piles were delivered by Thyssenkrupp Bautechnik, total area of approximately 4 000 m².

Delivery (2015-2016)

  • RR220/10 L=12 m pile elements approx. 34 000 m for approx. 2200 piles including rock shoes and bearing plates. Average pile length 17 m.

Co-operation partners

  • End customer: Akademiska Hus (County Council of Uppsala)
  • General contractor land: SH-Bygg
  • Foundations contractor: Hercules Grundläggning AB

Combi wall in BAVO Kademuren, Netherlands

Fast and reliable deliveries over a longer period of time

Läs mer

Combi wall in BAVO Kademuren, Netherlands

Fast and reliable deliveries over a longer period of time

Our solution

SSAB’s delivery of the primary piles provided with factory-welded interlocks for the combi walls in exact lengths. Solution for combi walls based on a high-strength steel grade S550J2H including welded interlocks. Overall project costs were cut by reducing the total amount of steel used. Savings were totally 385 ton. 

Customer case

The industrial area in the Rotterdam harbor had to be expanded. For this a new area was reclaimed from the sea and new harbors and customer specific quay walls had to be build.

"We chose SSAB as a supplier for the steel piles because it supplies good value for money and for the additional services it can provide", says H. Dries, project manager of the BAVO Kademuren Maasvlakte 2 project.

Delivery (2010-2011):

  • RR1200/13.0 mm, S550J2H, 2 126 ton (savings compared to 14.20 mm were 180 ton)
  • RR1200/17.6 mm, S550J2H, 125 ton (savings compared to 20.00 mm were 15 ton)
  • RR1200/14.2 mm, S550J2H, 1 842 ton (savings were 190 ton)
  • ø 1.620 x 20.00-24.00 mm, X-70, 550 ton
  • RR1000/12.5 mm, X-70, 295 ton
  • E21 interlocks 12.8 km and coating 674 m²

Co-operation partners:

  • Client: Maasvlakte 2 land reclamation project
  • Investor: Gemeentelijk Havenbedrijf Rotterdam
  • Main contractor: BAVO Kademuren (BAM and Volkerwessels)
  • Designer: BAM Infraconsult

RDs® and RR® piles in Bioproduct mill in Äänekoski, Finland

Extensive piles delivery with extremely flexible delivery schedule

Läs mer

RDs® and RR® piles in Bioproduct mill in Äänekoski, Finland

Extensive piles delivery with extremely flexible delivery schedule

Our solution

SSAB’s extensive delivery of RR and RDs piles enabled the customer flexible delivery planning in a demanding construction project. SSAB’s high strength steel piles solution met the demanding load bearing capacity demands cost-effectively and with minor soil displacement. All RD piles were delivered S550 steel grade. Piles manufactured to the customer-specific length enabled fast installation. Longest piles delivered were 26 m (RDs320/10). RR pile elements enabled fast and effective installation.

Customer case

Metsä Fibre, part of Metsä Group, builds a bioproduct mill in Äänekoski in the area of the existing pulp mill. The construction work is scheduled to be completed during the third quarter of 2017. The new bioproduct mill in Äänekoski is the largest investment of the forest industry in Finland. The total investment will amount to approximately EUR 1.2 billion.

The challenge for the customer, Metsä Fibre, was to find a reliable partner who can deliver large piling solution committed to flexible and prompt deliveries. Customer’s tight project schedule and limited storage possibilities at site set demands for extremely flexible delivery schedule. Customer’s challenge was to find a solution for demanding loads due to heavy structures of the mill machinery.

“Selection of pile dimensions for drilling was very successful. Amount of waste was minimum, practically almost no waste. Also the amount of splices were minimum, only couple splices”, says Taneli Murtoperä, Lujabetoni Oy.

Delivery (2015-2016):

  • RR piles: RR220/10 totally 26 km, 2 200 pcs, 1 400 t
  • RDs piles: RDs170/10, RDs170/12,5, RDs220/10, RDs220/12,5, RDs320/10 totally 40 km, 3 600 pcs, 2 000 t
  • Large diameter piles 200 t

Co-operation partners:

  • Client/Investor: Metsä Fibre
  • Piling contractor: Luja Betoni Oy
  • Driven piles operator: Niskasen Maansiirto Oy, Maasto-Seppo Oy, Junttapojat Oy
  • Drilled piles operator: Suomen Teräspaalutus Oy
  • Design: Sweco

RD® Pile wall in E18 Bommestad - Sky, Larvik tunnel, Norway

Preparing safe, stiff and watertight retaining walls for new tunnel

Läs mer

RD® pile wall in E18 Bommestad - Sky, Larvik tunnel, Norway

Preparing safe, stiff and watertight retaining walls for new tunnel

Our solution

SSAB's high strength steel RDs320/10 pilewalls were installed to secure 2 stiff and watertight parallell constructions through clay and moraine. Traffic could continue safely next to the site, and the soil could be excavated between the 2 walls.

Customer case

Statens vegvesen is building 7 km new E18 in Larvik, next to both existing highway and the vulnerable Lake Farris. One of the two tunnels in the project, Larvik tunnel, consist of 2 800 m tunnel in rock and 310 m tunnel in soil.

The challenge was to find a secure and reliable way to excavate the 310 m pit for tunnel in soil, without interfering with traffic or the lake. The soil being very complex with both soft clay and dense moraine, it was hard to solve this with only sheetpiles as retaining walls for the excavation.
Drilling of RDs320/10 with RM/RF interlocks, sealed with bituminous sealant, was done to required depths to secure stiff and watertight retaining walls, before excavation.

Delivery (2014-2015):

9600 m RDs320/10 incl. RM/RF-interlocks
5000 m RDs320/10
5800 m RDs220/12.5 with threaded sleeves
953 ton PU32 and 125 ton GU16N

Co-operation partners:

Project owner: Statens vegvesen
Main contractor: Skanska Norge AS
Piling contractor: Entreprenørservice AS
Geotechnical designer: Rambøll Norge AS

Two different methods for underpinning historical buildings in Sweden

Underpinning was needed to prevent excessive settlement of historical buildings in Stockholm and Gothenburg. In Pyramiden steel core piles were replaced by RD® piles with threaded splicing. In Högvakten RR® piles were used with two different techniques.

Läs mer

RD® and RDs® piles with threaded splicing in Kv Pyramiden, Sweden

Costs savings due to replacement of steel core to RD and RDs piles

Solution

SSAB delivered RD and RDs piles with threaded splicing to Betongsprutnings AB BESAB for large underpinning project to prevent excessive settlement of historical buildings. Cost savings were realized due to the replacement of steel core piles to RD piles and the use of high strength steel.

Customer case

Kv Pyramiden is located in Stockholm city center. Ten buildings established between 1898 and 1914 need underpinning to prevent excessive settlement. Each building was underpinned using 50 - 300 drilled RD piles with threaded splicing and each pile needed to be between 20 m and 25 m long to reach the bedrock. Drilling of piles was done with water powered drilling. 

Through the development of a custom made drop hammer, BESAB’s own design, the bearing capacity of the drilled RD piles could be measured even in the tightest of work spaces. This made it possible for BESAB, in agreement with the customer, to switch from steel core piles to RD piles. This change of piles lead to savings between 10% - 20% for the project. The usage of SSAB’s high strength steel piles in S550 grade contributed a lot to the savings.

Delivery (2016):

SSAB’s delivery content RD170/10, L=1-1,5 m RD170/12.5, L=1-1,5 m RDs170/10, L=1-1,5 m. In total 2 734 m = 2 666 pile elements.

Co-operation partners:

End customer: Svenska Bostäder
General contractor, land: Skanska Sverige AB
Foundations contractor: Betongsprutnings AB BESAB
Supplier of pile material: SSAB

 

RR® piles in Kv Högvakten, Sweden

Two different techniques for underpinning historical buildings

Solution

SSAB managed extensive delivery of 36 km of RR90 and RR115/6.3 short pile elements to Betongsprutnings AB BESAB. Project included underpinning of significant old buildings in the centre of Gothenburg.

Customer case

Four of Gothenburg’s oldest buildings needed underpinning due to excessive settlement. The underpinning used two different techniques. One technique was to core drill through the dry rubble, then drive RR piles on each side of the dry rubble and place a bearing beam on top of the driven RR piles which carries the weight of the building. All of the steel above ground was grouted for protection against corrosion.

The other technique used was zig-zag piling. Holes were core drilled with a slight incline through the wall and stone foundation. Then RR piles were driven through the holes to the hard bearing layer and cut from the bottom level of the foundation. Finally the holes in foundation were filled with concrete.

Delivery (2015-2016):

SSAB’s delivery content RR90, L=1-3 m and RR115/6.3, L=1-3 m. In total 36 000 m = 1 258 pile elements. Piles included rock shoes and bearing plates.

Co-operation partners:

End customer: City of Gothenburg, Higab
General contractor, land: F O Petersson & Söner Byggnads AB
Foundations contractor: Betongsprutnings AB BESAB
Supplier of pile material: SSAB

RRs® piles in Kiiruun school Somero, Finland

Up to 60 000 € savings when replacing with high strength RRs piles

Läs mer

RRs piles in Kiiruun school Somero, Finland

Up to 60 000 € savings when replacing with high strength RRs piles

Our solution

Higher load-bearing capacity and lower costs can be achieved when upgrading to RRs pile range and high-strength S550J2H steel grade. In this case SSAB’s technical support checked through the geotechnical and structural designs and made alternative calculations for RRs piles. The amount of pile points remained the same to prevent huge changes to other foundation designs. Also the total amount of piles by length remained the same. The change was made for pile dimensions.

Customer case

Somero is a small municipality at the South Western Finland. Old Kiiruun school was demolished due to health issues.

All originally designed steel piles in standard piling steel grade S440J2H were replaced with SSAB’s RRs piles. Customer saved up to 60 000 € in piling, save of steel material was about 84 tons.

The soil conditions at the site are demanding. There is very soft clay layer of 25 meters, a sand layer and finally a moraine layer. Piles were embedded all the way down to the moraine layer to ensure sufficient bearing capacity. The length of the piles was varying from 29 to 35 meters.

"Piling work at the site became easier and faster due to the smaller dimension of the piles. Handling of the piles was easy because the bundles are clearly lighter”, says Toni Sillanpää, Auranmaan Teräspaaluttajat Oy.

Delivery (2016):

RRs115/8, RRs140/8 and RRs140/10, totally 14 km, 373 t, 462 piles including bottom plates and bearing plates. Average pile length 30 m.

Co-operation partners:

Piling contractor: Auranmaan Teräspaaluttajat Oy
Designer: SWECO Rakennetekniikka Oy
Project owner: Somero municipality

Large diameter piles in Vanasadama Cruise Quay Tallinn, Estonia

Up to 46 m long steel pipe piles of two different wall thicknesses

Läs mer

Large diameter piles in Vanasadama Cruise Quay Tallinn, Estonia

Up to 46 m long steel pipe piles of two different wall thicknesses

Our solution

SSAB was able to produce and deliver special designed piles quickly and just in time taking into account any changes with the specification and time of delivery during the project.
Piles were delivered up to 46 m long and of two different wall thicknesses: 12.5mm lower part and 16.00mm upper part. All piles were fitted with an extra inside ring to increase pile bearing capacity. As it is a jetty type quay, delivery also included horizontal pipes.

Customer case

Tallinn is among the most popular destination for the cruise industry. To be able to handle the increasing number of cruise vessels the Vanasadama Cruise area had to be expanded and a new Cruise Quay had to be build.

The biggest challenge was to install very long 46 m inclined piles, 3:1, in one piece and within a very short time frame in open sea conditions.

“We chose SSAB to supply the steel piles because it provides good value, fast and flexible delivery, and because of its range of additional services” Rauno Kõiv, BMGS, Project manager

Delivery (2013):

  • 1016 x 12.50mm (S355J2H), 817 ton
  • 1016 x 16.00mm (S355J2H), 971 ton
  • 1220 x 12.50mm (S355J2H), 437 ton
  • 1220 x 16.00mm (S355J2H), 608 ton

Co-operation partners:

  • Client/Main contractor: BMGS Estonia branch
  • Investor: Port of Tallinn
  • Designer: Corson OÜ

RD® pile wall in Waitaki Power Station, New Zealand

Installation in restricted area with light equipment

Läs mer

RD® pile wall in Waitaki Power Station, New Zealand

Installation in restricted area with light equipment

Our solution

RD® pile wall system was installed with relatively small and light equipment. Also installation involved less drilling work than initial solution with secant piles (no soft piles to drill out).
SSAB delivered complete retaining wall structures including steel pipe piles with welded interlocks

Customer case

Old sluice pier of Waitaki Power Station had been undermined. This pier separates the sluice water drawn from the dam and the turbine tailrace. The access to the pier is very restricted and confined causing challenges regarding the installation with heavy equipment.

Delivery (2014-2015):

RD320/8 with RM/RF interlocks L= 15 m, in total 1 000 m

Co-operation partners:

Designer and general contractor: McConnell Constructors Ltd

RD® pile wall for tunnel to Stortinget building, Norway

Cramped city centre with restrictions on drilling and minimum space

Our solution

SSAB‘s RD pile walls was the best suitable solution for making retaining walls very close to existing stores and office buildings.

Customer case

Underneath the street Nedre Vollgate, a 250 m long supply tunnel for a new post- and goods reception for Stortinget (the Parliament) is to be build.

The challenges when building a tunnel below an existing street in Oslo are many. The area is cramped with little room to work, tight access and difficulties to store materials and equipment. Drilling is restricted to nights (after office hours) because of business running as usual in adjacent buildings.

A solution was needed for establishing retaining walls through varying soil conditions and securely into bedrock, very close to existing buildings. By using RD pile walls this is possible. Later the street can be excavated, the supply tunnel can be build and the street can be reestablished on top of the tunnel.

The designer Multiconsult AS found RD400/10 with RM/RF-interlocks to be best solution for this task, drilled 2 m into bedrock, and with interlocks sealed with Pertex. The total number of piles is currently predicted to be 436, and the lengths vary from 9 to 14 m.

Delivery (2016):

  • 5000 m RD400/10 S355J2H incl. RM/RF-interlocks with Pertex, and ringbits from Robit welded onto the 436 piles

Co-operation partners:

  • Project owner: Stortinget
  • Main contractor: Veidekke ASA
  • Piling contractor: Hallingdal Bergboring AS
  • Geotechnical designer: Multiconsult AS

RD® pile wall in Pasila Tripla, Finland

Reliable and watertight retaining wall in demanding soil conditions and busy urban environment with fast installation

Läs mer

RD® pile wall in Pasila Tripla, Finland

Reliable and watertight retaining wall in demanding soil conditions and busy urban environment with fast installation

Our solution

SSAB‘s RD pile wall solution enabled fast installation with tight tolerances. Accuracy and speed in addition to water tightness made RD pile wall best solution for the customer. Installation method was also least risky for the surroundings as removing the clay with auger creates little to no spatter. Piles were transported full-length sections. Exceptional length of the piles was up to 33,5 m (8,5 t).

Customer case

Pasila Tripla is three-block retail, office and housing complex to be built in Pasila district close to the city center of Helsinki. It will be completed in stages by the early 2020s.

Customer’s challenge was to find a watertight retaining wall solution to surround the 640 000m3 excavation for the garage. Location is critical right by a bridge with foot traffic, railway track and busy Pasilankatu street. Delivery and installation speed were critical for the customer: it was important to have piles delivered in one piece to avoid additional welding at site. The retaining wall cuts through groundwater layers, which exerts an enormous pressure on the underground structures making water-proofing the retaining wall demanding.

Delivery (2015-2016):

  • SSAB RD pile walls
  • 754 pcs RF/RM-interlocked drilled piles RD700/14.2, 16 700 m in total
  • 60 pcs RF/RM-interlocked drilled piles RD400 /12.5, 1 300 m in total
  • 60 pcs structural pipes RD323/12.5, 1 300 m in total
  • Casings for anchors: RDc140/5.0 + RDc170/5.0

Co-operation partners:

  • Client/Project owner: YIT Rakennus Oy
  • Main contractor: Keski-Suomen Betonirakenne Oy
  • Drilling contractor: Fort Ehitus OÜ and YIT Rakennus Oy
  • Drilling consultant: Ilmi Solutions Oy
  • Drill bit supplier: Robit Oyj
  • Design: Ramboll Finland Oy

RD® pile wall in Hedemora kommun , Sweden

Very satisfying solution in limited space and soft ground conditions

Läs mer

RD® pile wall in Hedemora kommun, Sweden

Very satisfying solution in limited space and soft ground conditions

Our solution

Demand from customer was total construction. Dimensioning of piles according to existing standards. Safety was of the highest concern. Usage of RD-wall due to both soil conditions and aesthetics.

Customer case

The project was in Hedemora and regarded reinforcement of a stone wall. The stone wall had started to disintegrate and needed reinforcement.

Limited space and soft ground presented great challenges. The RD-pile wall-solution smoothly overcame the challenges, the toughest one being when the currently drilled pile started to pull down the pile next to it.

This was also the first time Svevia and Foundation Drilling Sweden AB used an RD pile wall for a project and the end result is more than satisfying.

Delivery (2015-2016):

SSAB’s delivery content RD320/10, L=9 m with RM/RF interlocks. 558 m² = 62 piles, including pressure plates

Co-operation partners:

End customer: Hedemora kommun
General contractor, land: Svevia
Foundations contractor: Foundation Drilling Sweden AB
Supplier of pile material: SSAB

Pipeline in Hunstok-Akersvann, Stokke, Norway

Long and heavy pipes delivered promptly within short time frame

Läs mer

Pipeline in Hunstok-Akersvann, Stokke, Norway

Long and heavy pipes delivered promptly within short time frame

Our solution

SSAB is able to produce and deliver by trucks coated pipes quickly and just in time taking into account any changes with time of delivery during the project.

SSAB’s delivery content includes 15 km of coated DN1000 water pipes and fittings. Delivery consist of 16 m long and 5 tons pipes and pipe fittings to the site. All pipes and pipe fittings are externally and internally coated. SSAB’s OV welded joint facilitates installation and allows 2,0 degree bends at joints.

Customer case

Vestfold Vann IKS has been established 1968 and is owned together by 10 municipalities in Vestfold county in south part of Norway. The mission of Vesfolf Vann IKS is to offer the partners drinking water of good quality.

The biggest challenge is to transport and move 16 m long and 5 tons heavy pipes to wet fields before installation within a very short time frame and in very variable winter conditions.

"We chose SSAB to supply the coated steel pipes and fittings because it provides good quality, and fast and flexible delivery to the site by trucks“, says Einar Klavenes, Vesfold Vann, Project manager.

Delivery (2014-2017):

1016 x 8,8 mm – St37,0 – 15000 m, 3300 tonnes (steel)

Co-operation partners:

Investor: Vestfold Vann IKS
Partner: Brødrene Dahl AS
Designer: COWI
Main contractor: Arne Olav Lund AS

Pipeline in Kaupintie-Lapinmäentie, Helsinki, Finland

Water mains produced and delivered parallel to several locations and modifications

Läs mer

Pipe line in Kaupintie-Lapinmäentie, Helsinki, Finland

Water mains produced and delivered parallel to several locations and modifications

Our solution

SSAB is able to tailored produce and deliver by trucks coated pipes quickly and just in time taking into account any changes with time of delivery during the project.

This SSAB’s delivery content includes 1500 m of coated DN600-800 water pipes and fittings. Delivery consist of mainly 8 m long pipes and butt joint or DIN/G-welded joints. All pipes and pipe fittings are externally and internally coated. Externally 3 mm HDPE-coating was used to ensure very long lifetime against corrosion. Internally was used cement mortar lining.

Customer case

Helsinki Region Environmental Services Authority (HSY) is a municipal body, which produces waste management and water services on the Helsinki Metropolitan Area.

The biggest challenge is to produce and deliver pipes and fittings parallel to several construction locations and modifications during installation.

Delivery (2015-2016):

610 x 8 mm – P235GH – 300 m, 35 tonnes (steel)
813 x 8,8 mm – P235GH – 1000 m, 175 tonnes (steel)

Co-operation partners:

Investor: HSY
Designer: Ramboll
Main constructor: Graniittirakennus Kallio Oy

Threaded RD270 in Uddevalla, Sweden

Fast and easy piling without welding in project Skeppsholmspiren

Läs mer

Threaded RD270 in Uddevalla, Sweden

Fast and easy piling without welding in project Skeppsholmspiren

Our solution

SSAB’s mechanical splices also to larger RD pile sizes answer the increasing customer demand. Threaded pile element RD270 was first used in this project. Mechanical splicing eliminates the need for splice welding at site. When splicing of a pile is done mechanically, many weather conditions related problems can be avoided at the construction site. The high-quality of the splicing remains good in all weather conditions.

Customer case

Project Skeppsholmspiren was located in harbor in Uddevalla. Uddevalla is situated on the Swedish West Coast, north of Gothenburg and south of Oslo.

Due to the demanding conditions at site, customer chose to use drilled steel piles. Original design with concrete piles was rejected because the inclination of surface of the bedrock was too steep. The solution was RD270/12.5 piles with threaded mechanical splices. The bottom elements of piles were 14 m long and the length of the upper pile elements varied. Piling was managed to finish couple days earlier than planned. Also work safety at site was improved compared to welding.

“We were very satisfied with the product. The piles were easy to handle at the site since there were no heavy sleeves. Time savings were remarkable when there was no need for welding outside. Thanks to the mechanical splicing, the weather conditions didn’t play any role in the progress of the piling work. Threads worked well in all conditions”, says Victor Gillholm, Skanska Grundläggning.

Delivery (2016):

RD270/12.5, 876 m, 35 pcs, 72 t

Co-operation partners:

Project owner: Uddevalla harbour
Piling contractor: Skanska Grundläggning
Designer: Skanska Teknik
Piling operator: Foundation Drilling Sweden

Break water in Ust-Luga, Russia

Pile/pile wall with special interlocks and inclined piles

Läs mer

Break water in Ust-Luga, Russia

Pile/pile wall with special interlocks and inclined piles

Our solution

SSAB's pile/pile wall with special interlocks and inclined piles was a reliable solution in terms of availability and schedule.

All piles for each stage have been loaded in dedicated vessels for delivery straight into Ust-Luga.

Customer case

The harbor in Ust-Luga need to be protected from the sea. The break water will be completed in stages between 2013 and 2017.

The challenge for the customer was to build a break water in a short period of time due to challenging ice conditions.

“We  have chosen SSAB because of the convenient location of the pipe production and short delivery time” Tatjana Detzel, TKBT

Delivery(2014-2016):

SSAB pile / pile wall and inclined piles
650 pcs LPB180 interlocked piles ø 1020 x 12,00 mm, 5 600 t, 14 800 m in total
475 pcs ø 1220 x 12,00 mm, 4 100 t, 11 400 m in total

Co-operation partners:

Client: ThyssenKrupp Bautechnik GmbH
Developer: Rosmorport

RD® pile wall in E18 Bommestad - Sky, Farris bridge, Norway

Deep foundations in moraine and close to highway and Lake Farris

Läs mer

RD® pile wall in E18 Bommestad - Sky, Farris bridge, Norway

Deep foundations in moraine and close to highway and Lake Farris

OUR SOLUTION

SSAB's RD pile walls, in combination with sheet piles, was the best way to make “boxes” for 8 of the 10 foundations, close to the highway and in coarse and dense soil.

CUSTOMER CASE

Statens vegvesen is building 7 km new E18 in Larvik, next to both existing highway and the vulnerable Lake Farris. The new Farris Bridge is a separate contract with all its complexity. The bridge is 570 m long and 28 m wide, consisting of 10 foundations.

The challenges consist of different aspects: the vicinity to existing highway and Lake Farris, and the depths to bedrock (20-80 m) in combination with the varying soil conditions.

SSAB’s customer made 8 “boxes” with different combinations of RD pile walls and sheet piles depending on soil conditions. Within each “box” RR piles and drilled piles were installed to take the future loads of the new bridge.

Delivery (2014-2015):

4500 m RD400/8 incl. RM/RF-interlocks
1800 m RR900/20 incl. 94 pcs. rockshoes
3200 m RD300/6.3 casings
128 ton GU21N and 602 ton AZ18

Co-operation partners:

Project owner: Statens vegvesen
Main contractor: Bilfinger
Piling contractors: Kynningsrud Fundamentering AS and Hallingdal Bergboring AS

Pipeline in Upplands Bro-Sigtuna, Sweden

Tailored DN600 water mains delivered quickly and just in time

Läs mer

Pipeline in Upplands Bro-Sigtuna, Sweden

Tailored DN600 water mains delivered quickly and just in time

Our solution

SSAB is able to tailored produce and deliver by trucks coated pipes quickly and just in time taking into account any changes with time of delivery during the project.

This SSAB’s delivery content includes 3000 m of coated DN600 water pipes and fittings. Delivery consist of mainly 16 m long pipes and DIN/G-welded joints. All pipes and pipe fittings are externally and internally coated.

Customer case

Norrvatten is a municipal council owned by 14 different urban municipalities in the northeast sector of Stockholm. It produces and distributes drinking water of the highest quality. 

The biggest challenge during project is to produce and deliver pipes and fittings parallel to several construction locations and modifications during installation.

“We chose SSAB for a supplier of coated pipes and fittings, because it offers very good quality and tailor-made fittings for whole project“, says Christer Thoursie, Norrvatten, Construction manager.

Delivery (2015-2016):

610 x 8 mm – P235GH – 3000 m, 356 tonnes (steel)

Co-operation partners:

Investor: Norrvatten
Designer: Structor
Main constractor: Peab
 

RD® pile wall in Vojmsjön dam, Sweden

A tight time frame and challenging conditions for water tightness

Läs mer

RD® pile wall in Vojmsjön dam, Sweden

A tight time frame and challenging conditions for watertightness

Our solution

SSAB delivered an RD® - pile wall which is developed to ensure reliable results corresponding to design specifications in even the most difficult conditions.

The RD® pile wall structure is installed by drilling, and replaces separate retaining wall and foundation structures, minimizing build times and generating savings in overall project cost. In addition, SSAB´s lock type – RM/RF – ensures the best possible watertightness in wall structures.

SSAB delivered a 170 m long drilled steel pile wall (totally 1680 m2) with an interlock system. The piles are attached to each other by interlocking sections assuring the wall the best possible watertightness.

Customer case

The Vojmsjön reservoir dam receives large amount of melt water from the surrounding mountains. At peak flow, the dam is filled in less than a week. To give a sealing for the dam the SSAB RD® pile wall with interlocking system was utilised to assure the watertightness. As the spring flood can be severe in Lapland the timeframe for the dam rehabilitation project was quite tight.

Delivery (2014):

RD320/8 pile wall with RM/RF interlocks 4600 m (1680 m2)

Co-operation partners:

Client/Contractor: Lemminkäinen Sverige AB
Consultants: Sweco AB and GeoMind


Large diameter piles in Extension of deep quay in Kokkola, Finland

Extensive steel structure delivery fast and reliably

Läs mer

Large diameter piles in Extension of deep quay in Kokkola, Finland

Extensive steel structure delivery fast and reliably

Our solution

Effective utilization of SSAB’s sub contractor network enabled us to serve all customer’s steel structure needs. Customer received all needed steel structures for the project from one reliable supplier fast and accurately.

New combi wall solution was used, in which the steel piles were manufactured from extra high strength steel with high load bearing capacity. Piles were the longest (33.5 m) and heaviest (20 tons/ each) that had been delivered in Finland so far.

Customer case

Investment in Kokkola harbour included extension of deep quay: Silverstone quay 1 and Silverstone quay 2. Investment enables increasing the capacity of the harbour. New lay-out of the port area has been designed to support the competitive pricing of Port of Kokkola. 

The challenge for the customer was to find a partner to deliver all needed steel structures for harbour piers. Fast and accurate delivery was demanded.

1st Delivery (2009):

Steel piles for combi wall: RR1200/16 (X70), 1 600 m and E22 interlocks welded 2 600 m
Sheet piles for combi wall: Larssen 43, 220 tons
Anchor piles: Gewi 63.5, 1 400m, L= 33.0 m
Piles for crane rail: RR500/12.5 (S355J2H), 800 m

2nd Delivery (2011-2012):

Steel piles for combi wall: RR1200/15 (S550J2H), 1 600 m and E22 interlocks welded 2 700 m

Co-operation partners:

Client/Main contractor: Terramare Oy (1st delivery), YIT Rakennus Oy (2nd delivery)
Investor: Kokkola harbour
Design: Insinööritoimisto Pitkälä Oy

Dolphin piles in VSF Jetties 1 & 2 BP Rotterdam, Netherlands

Renovation fenders Jetties 1 & 2

Läs mer

Dolphin piles in VSF Jetties 1 & 2 BP Rotterdam, Netherlands

Renovation fenders Jetties 1 & 2

Our solution

SSAB's supplied the ready to be installed Dolphins just in time on site. Dolphins has been re-designed in higher steel grade (Optim 500ML) and has been supplied including coating. Also loose pile heads have been supplied for further processing by the customer.

Customer case

The existing jetties 1 & 2 need to be renovated to suit future vessel sizes. The work is executed in different phases and starts with demolishing the existing jetties. Each phase needs to be executed within only 3 weeks. As part of phase 1 two new dolphins need to be installed.

Absolutely essential is that the dolphins are supplied as agreed since heavy and expensive equipment has been scheduled according to the planning.

“We selected SSAB as the preferred supplier because they were able to delivery the dolphins within the requested time frame and budget”, says Arjan Joling, project manager Volker Staal en Funderingen b.v.

Delivery (2010):

2 pcs. ø 2800,0 x 24.00 mm, S355J2H, L = 3700 mm
2 pcs ø 2800.0 x 30.00/40.00/60.00/40.00/24.00 mm, Optim 500ML, L = 44600 mm, weight 125553 kg
Coating 25 100 mm

Co-operation partners:

Client: BP Raffinaderij Rotterdam B.V.
Main contractor: Volker Staal en Funderingen b.v.

Large diameter piles in BAM Neste Oil Jetty Rotterdam, Netherlands

Extremely long piles fast and reliably

Läs mer

Large diameter piles in BAM Neste Oil Jetty Rotterdam, Netherlands

Extremely long piles fast and reliably

Our solution

SSAB's supplied extremely long piles including coating fast and reliable. SSAB’s delivery included in total 1,4 km large diameter steel piles.

Coating system: Shot blasted as per Sa 2½ 1 layer Sigmacover primer , 75 µm (grey) 1 layer Sigmacover DTM coating 150 µm (light grey) 1 layer Sigmacover DTM coating , 150 µm (black RAL 9017

Customer case

Neste Oil built a renewable diesel plant in Rotterdam completed in 2011. The challenge for the customer was to find a partner with the ability to deliver extremely long piles up to 46 meter long according to customer’s needs fast and reliably.

Delivery (2010-2011):

RR650/12.8, S355J2H, L=15.3…45.3 m (156 ton) incl. coating 6.3…22.9 m (40…70%)
RR900/16.4, S355J2H, L=33.7…45.9 m (229 ton) incl. coating 22.9 m (50…70%)

Co-operation partners:

Investor: Neste Oil
Main contractor: Technip Italy
Sub contractor: BAM Infra Zuidwest

RD® pile wall in Center of Kalasatama REDI, Finland

Watertight and permanent retaining wall in sea landfill on a tight schedule

Läs mer

RD® pile wall in Centre of Kalasatama REDI, Finland

Watertight and permanent retaining wall in sea landfill on a tight schedule

Our solution

SSAB's watertight RD pile wall was a reliable solution in terms of technical elements and schedule. SSAB's watertight RD pile wall was used to ensure and enable safe and rapid building of wide underground spaces and access tunnels that reach ten meters below sea level.

Customer case

New residential area of Kalasatama, REDI, consist of six residential towers, one office and one hotel tower. At the base of the towers will be the largest shopping and lifestyle centre in Helsinki’s inner city. Redi is located at the intersection of three major arterial roads by the sea. The shopping centre opens in 2017, and the first residential tower will be ready for occupants around 2018. By 2022, REDI will be completed.

The challenge for the customer was to build a watertight and permanent retaining wall in the sea landfill on a tight schedule. Also, the connection between the wall and rock had to be secure.

“The product and solution complied well with the technical and functionality requirements specified for them. We are particularly satisfied with the fast and accurate deliveries by SSAB. Also, needs for changes during the work were responded to quickly. The deliveries worked perfectly in this project”, says Pentti Väyrynen, Destia Oy.

1st Delivery (2011-2012):

SSAB RD pile walls for access tunnels 2 and 4
356 RM/RF-interlocked drilled piles RD610/12.5, 2 600 m in total

2nd Delivery (2015-2016):

SSAB RD pile walls for access tunnels 1 and 3
466 RM/RF-interlocked drilled piles RD610/12.5, 5 200 m in total

Co-operation partners:

Client/Infrastructure construction: Destia Oy
Developer: SRV Oy
Retaining wall subcontracting: YIT Oyj (1st delivery)
Piling subcontracting: Sotkamon Porakaivo Oy (1st delivery), ITS Vahvistus (2nd delivery)
Design: Sito Oy