Strenx Tube 960MH

Strenx® Tube 960MH

Advanced high-strength structural hollow sections

Strenx® Tube 960MH is an HF-welded cold-formed structural hollow section made of hot-rolled high-strength steel with a minimum yield strength of 960 MPa.

Its high strength combined with naturally stiff form of welded hollow section enables construction of stronger and lighter structures. Strenx® Tube 960MH meets or exceeds the requirements of EN 10219-3 (2020). Typical applications include load-bearing structures in the lifting, handling and transportation segments.

Strenx® Tube 960MH is available in circular, square and rectangular shapes. Other shapes and sizes are available upon request.

The maximum length of the tubes is 12-18 meters, depending on the size. Longer or cut-to-length tubes are available upon request.

It is not recommended to hot dip galvanize Strenx® Tube 960MH hollow sections.

Dimensionsintervall

Strenx® rör 960MH kan som cirkulär, kvadratiskt eller rektangulär form. 

Cirkulärt 114.3 - 244.5 mm 
Fyrkantigt 100x100 - 200x200 mm 
Rektangulärt 120x80 - 250x150 mm 
Väggtjocklek 4.0 - 6.0 mm
Fabrikslängd    6 000 - 12 000/18 000 mm

Andra former och storlekar finns på begäran.

Tillgängliga standarder

EN 10219

Välj form för att visa egenskaper