Strenx Tube 700MLH
Advanced high-strength structural hollow sections

Strenx® Tube 700MLH

Advanced high-strength structural hollow sections

Strenx® Tube 700MLH is an HF-welded cold-formed structural hollow section made of hot-rolled high-strength steel with a minimum yield strength of 700 MPa.

Its high strength combined with naturally stiff form of welded hollow section enables construction of stronger and lighter structures. Strenx® Tube 700MLH meets or exceeds the requirements of EN 10219-3 (2020) and it is CE marked according to EN 1090-2. Typical applications include load-bearing structures in the lifting, handling and transportation segments, especially in conditions that require extremely good toughness.

Strenx® Tube 700MLH is available in circular, square and rectangular shapes. Other shapes and sizes are available upon request.

The maximum length of the tubes is 12-18 meters, depending on the size. Longer or cut-to-length tubes are available upon request.

Hot dip galvanizing Strenx® Tube 700MLH hollow sections may lead to cracking. Please consult SSAB Tech Support prior galvanization.

Dimensionsintervall

Strenx® rör 700MLH kan fås i cirkulär, kvadratisk eller rektangulär form. 

Cirkulärt 42.4 - 323.9 mm 
Fyrkantigt 40x40 - 300x300 mm 
Rektangulärt 50x30 - 400x200 mm 
Godstjocklek 3.0 - 10.0 mm
Fabrikslängd 6 000 - 12 000/18 000 mm

Andra former och storlekar finns på begäran.

Tillgängliga standarder

EN 1090-2

EN 10219

Välj form för att visa egenskaper