Strenx® Section 650MC
Спецификации
Спецификации
Strenx® Section 650MC is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 650 MPa.
Its high-strength combined with naturally stiff form enables construction of stronger and lighter structures. Typical applications include demanding load-bearing structures in the lifting, handling and transportation segments.
Strenx® Section 650MC is available as U-section. Other shapes and variations are available upon request. The maximum length of the sections is 21 meters, cut-to-length sections are available upon request.
Strenx® Section 650MC is available as U-section. Other shapes and variations are available upon request.
тип продукт | U-Section |
---|---|
Bottom length (ммin) | 50 - 4001.969 - 15.748 |
Side length (ммin) | 30 - 2001.181 - 7.874 |
Толщина стенок (ммin) | 2.5 - 8.00.098 - 0.314 |
макс длина (ммin) | 12000826.770 |
Толщина (ммin) |
Предел текучести ReH 1) (мин МПаksi) |
Предел прочности Rm (МПаksi) |
Относительное удлинение A80 (min %) |
Относительное удлинение A5 (%) |
Мин. внутренний радиус загиба на 90° |
---|---|---|---|---|---|
2.50 - 3.000.098 - 0.118 | 65094 | 700 - 850101 - 123 | 12 | — | 0.8 x t |
3.01 - 6.000.118 - 0.236 | 65094 | 700 - 850101 - 123 | — | 14 | 1.2 x t |
6.01 - 8.000.237 - 0.314 | 65094 | 700 - 850101 - 123 | — | 14 | 1.5 x t |
Механические свойства тестируются в продольном направлении.
1) Вместо величины ReH допускается применение значения Rp0.2. При толщине >8 мм допускается снижение минимального предела текучести на 20 МПа.
продукт | Мин. работа удара для продольных образцов Шарпи 10 x 10 мм с V- образным надрезом 1) |
---|---|
Strenx® Section 650MC | 27 J / -40 °C20 ft-lbs / -40 °F |
1) Испытания на удар проводятся по стандарту EN ISO 148-1 при толщине ≥ 6 мм. Заданное минимальное значение относится к полноразмерным образцам.
C (max %) |
Si (max %) |
Mn (max %) |
P (max %) |
S (max %) |
Altot (min %) |
Nb (max %) |
V (max %) |
Ti (max %) |
---|---|---|---|---|---|---|---|---|
0.12 | 0.21 | 2.00 | 0.025 | 0.010 | 0.015 | 0.090 | 0.20 | 0.15 |
If the material is to be hot-dip galvanized according to category A or category B in EN 10149-2 this must be specified at the time of order.
Sum of Nb, V and Ti = max 0.22%
The steel is grain refined.
Толщина (ммin) | 2.5 - 8.00.098 - 0.314 |
---|---|
Тип. CET(CEV) | 0.22 (0.34) |
Подробнее см. в условиях гарантии Strenx® на сайте www.ssab.com.
The sections are roll formed from thermomechanically rolled steel.
Strenx® Section has good weldabilility, including corner region, and it is suitable for thermal cutting. All the common welding methods are suitable with matching or undermatching consumables.
Sections can also be sawed and machined with regular tools. Bending of the sections is also possible, please contact Tech Support for further instructions. For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the product.