    Общее описание продукции

    Normalized or normalized rolled structural steel heavy plate. SSAB Multisteel HSD and HSE are hot rolled hull structural steel for general marine steel constructions. HS = Hull Structural – D and E = impact strength class.

    Exceeding the requirements of several classification societies rules, SSAB Multisteel HS is a versatile structural steel for shipbuilding. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

    SSAB Multisteel HS exceeds several steel standards and is available as six societies rules: DNV (NV), Lloyd's Register EMEA (LR), American Bureau of Shipping (AB), Bureau Veritas (BV), Registro Italiano Navale (RINA), Russian Maritime Register of Shipping (PC) and also possible to certify to EN 10025-2 S355K2+N.

    Maximum four (4) different grade if one of them is AB. Otherwise maximum three (3) grades in one plate. Combinations e.g NVD36/ABDH36N/BVDH36/PCD36 or NV D36/BV DH36/S355K2+N. Please enquire for suitable combination before placing the order.

    CE marking:

    SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-1 and EN 10025-2. The CE marking is marked on an extra page of inspection certification 3.1 for S355K2+N. CE marking can be given only if S355K2+N is one of the steel grades in the combination.

    Типоразмерный ряд

    SSAB Multisteel HSD is available in thicknesses of 5.00 - 150.00 mm.

    SSAB Multisteel HSE is available in thicknesses of 5.00 - 150.00 mm.

    (If PC is involved in the combination max thickness is 100 mm.)

    Механические свойства

    Скрыть/показать определённые столбцы Редактировать
    Выбрать столбцы для отображения
      Толщина
      (мм)
      Предел текучести
      (мин МПа)
      Tensile strength
      (МПа)
      Относительное удлинение A5
      (min %)
      5.00 - 100.00 355 490 - 620 21
      100.00 - 150.00 355 490 - 600 21
      Сравнение параметров

      Выберите один параметр для сравнения

      Сравнение

        The mechanical properties are tested transverse to the direction of rolling.

        Ударная вязкость

        Скрыть/показать определённые столбцы Редактировать
        Выбрать столбцы для отображения
          Толщина
          (мм)
          Мин. работа удара для продольных образцов Шарпи 10 x 10 мм с V- образным надрезом
          SSAB Multisteel HSD 5.00 - 50.00 34 J / -20 °C
          50.01 - 70.00 41 J / -20 °C
          70.01 - 150.00 50 J / -20 °C
          SSAB Multisteel HSE 5.00 - 50.00 34 J / -40 °C
          50.01 - 70.00 41 J / -40 °C
          70.01 - 150.00 50 J / -40 °C
          EN 10025-2 S355K2+N 5.00 - 150.00 40 J / -20 °C
          Сравнение параметров

          Выберите один параметр для сравнения

          Сравнение

            The impact test is made longitudinally to the rolling direction in compliance with society rules and EN 10025-2.

            Химический состав (ковшевая проба)

            Скрыть/показать определённые столбцы Редактировать
            Выбрать столбцы для отображения
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Nb
              (max %)
              0.18 0.50 1.60 0.025 0.020 0.05
              Сравнение параметров

              Выберите один параметр для сравнения

              Сравнение

                Углеродный эквивалент CEV

                Скрыть/показать определённые столбцы Редактировать
                Выбрать столбцы для отображения
                  тип продукт If only hull structural steel If only hull structural steel If S355K2+N is in the combination If S355K2+N is in the combination
                  Толщина (мм) 5.00 - 60.00 60.01 - 150.00 5.00 - 60.00 60.01 - 150.00
                  CEV (Макс %) 0.45 0.49 0.45 0.47
                  Сравнение параметров

                  Выберите один параметр для сравнения

                  Сравнение

                    Допуски

                    All tolerances according to society rules and EN 10029 – thickness ¾ class B.

                    Flatness tolerance 6 mm/m.

                    Surface according to EN 10163-2 Class A subclass 1 or 3 (when RINA or when thickness is over 100 mm).

                    Условия поставки

                    SSAB Multisteel HSD

                    Typically (can be chosen by SSAB)

                    Normalized rolled (thickness 5.00 - 40.00 mm)

                    Normalized (thickness 40.01 - 150.00 mm)

                    SSAB Multisteel HSE

                    Normalized (thickness 5.00 - 150.00 mm)

                    Coating

                    Shot blasted & primed surface is available upon request.

                    Certificates

                    Mill sheet for hull structural steel according to Classification Society grades.

                    EN 10204-3.1+CE for S355K2+N EN 10025-2 (if chosen to be in the combination).

                    Рекомендации по обработке

                    Welding:

                    Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                    Needed working temperatures for thick plates please consult SSAB Tech Support.

                    Forming:

                    SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                    Guaranteed minimum bending radius for all directions is 2 x t up to 30 mm thick plate where t = plate thickness.

                    Heat treatment:

                    Recommendations for stress relieving and normalizing.

                    Stress relieving 550 – 600°C (target 580°C)

                    2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                    Normalizing 900 – 940°C (target 920°C)

                    1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                    Информацию об обработке можно найти в брошюрах SSAB на сайте www.ssab.com или связаться с технической поддержкой.