    General Product Description

    GreenCoat RWS Pural BT color coated steel is available in matt finish. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

    GreenCoat RWS Pural BT offers the highest level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).

    GreenCoat RWS Pural BT color coated steel provides excellent corrosion resistance (RC5), gloss retention and color fastness (Ruv5). GreenCoat RWS Pural BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

    Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.

    GreenCoat RWS Pural BT complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    GreenCoat and Pural are trademarks of the SSAB group of companies.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Matt
      Gloss < 5
      Minimum inner bending radius 0.5 x sheet thickness
      Scratch resistance 30 N
      Lowest forming temperature -15 °C
      UV radiation resistance RUV5
      Corrosion resistance 1) RC5
      Stain resistance Good
      Highest operating temperature 100 °C
      Coating thickness, nominal (primer + top coat) 40 µm
      Coating structure Structured
      Steel designation 2) PLX , FAX , S280GD, DX51D, DX52D/RWS , DX54D 3)
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.50 mm
      Steel width 2) 1000 - 1500 mm 4)
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Matt
        < 5
        Technical Properties
        Minimum inner bending radius
        Matt
        0.5 x sheet thickness
        Technical Properties
        Scratch resistance
        Matt
        30 N
        Technical Properties
        Lowest forming temperature
        Matt
        -15 °C
        Technical Properties
        UV radiation resistance
        Matt
        RUV5
        Technical Properties
        Corrosion resistance 1)
        Matt
        RC5
        Technical Properties
        Stain resistance
        Matt
        Good
        Technical Properties
        Highest operating temperature
        Matt
        100 °C
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Matt
        40 µm
        Technical Properties
        Coating structure
        Matt
        Structured
        Technical Properties
        Steel designation 2)
        Matt
        PLX , FAX , S280GD, DX51D, DX52D/RWS , DX54D 3)
        Technical Properties
        Zinc coating
        Matt
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Matt
        0.50 mm
        Technical Properties
        Steel width 2)
        Matt
        1000 - 1500 mm 4)

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D, DX52D/RWS fulfills the requirements of EN 10346 DX52D.

        4) Max width 1420 mm for color RR33 / SS0015.

        Colors

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
        5 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat RWS Pural BT

        Mountain Grey

        RR23 / SS0036

        Matt

        Slate Grey

        RR2H3 / SS0534

        Matt

        Nordic Night Black

        RR33 / SS0015

        Matt

        Walnut Brown

        RR32 / SS0387

        Matt

        Chestnut Brown

        RR887 / SS0435

        Matt

        The product may have slight tonal difference between batches and especially if their time of production differs significantly.

        Reverse Side Coating

        Coating is applied in same color on both sides of the sheet.

        The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

        Reverse side stamping is not applicable for double sided products.

        Contact Information

        www.ssab.com/contact