GreenCoat RWS Pro

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    GreenCoat RWS Pro color coated steel is available in regular finish and offers a wide range of colors inspired by Nordic nature.

    GreenCoat RWS Pro offers a high level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).

    GreenCoat RWS Pro color coated steel is optimized for weather and wear resistance. It provides good protection against corrosion (RC5) and mechanical abrasion as well as very good gloss retention and color fastness. GreenCoat RWS Pro possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

    Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.

    GreenCoat RWS Pro complies with current REACH regulations and is fully chromate-free.

    SSAB’s color coated steels are all manufactured according to EN 10169.

    Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Technical Properties Regular
      Gloss 40
      Minimum inner bending radius 0.5 x sheet thickness
      Scratch resistance 30 N
      Lowest forming temperature -15 °C
      UV radiation resistance RUV3
      Corrosion resistance 1) RC5
      Stain resistance Very good
      Highest operating temperature 100 °C
      Coating thickness, nominal (primer + top coat) 35 µm
      Coating structure Structured
      Steel designation 2) FAX, PLX 3)
      Zinc coating 275 g/m2
      Min steel thickness 2) 0.50 mm
      Steel width 2) 1000 - 1500 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Technical Properties
        Gloss
        Regular
        40
        Technical Properties
        Minimum inner bending radius
        Regular
        0.5 x sheet thickness
        Technical Properties
        Scratch resistance
        Regular
        30 N
        Technical Properties
        Lowest forming temperature
        Regular
        -15 °C
        Technical Properties
        UV radiation resistance
        Regular
        RUV3
        Technical Properties
        Corrosion resistance 1)
        Regular
        RC5
        Technical Properties
        Stain resistance
        Regular
        Very good
        Technical Properties
        Highest operating temperature
        Regular
        100 °C
        Technical Properties
        Coating thickness, nominal (primer + top coat)
        Regular
        35 µm
        Technical Properties
        Coating structure
        Regular
        Structured
        Technical Properties
        Steel designation 2)
        Regular
        FAX, PLX 3)
        Technical Properties
        Zinc coating
        Regular
        275 g/m2
        Technical Properties
        Min steel thickness 2)
        Regular
        0.50 mm
        Technical Properties
        Steel width 2)
        Regular
        1000 - 1500 mm

        1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

        2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

        3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.

        Colors

        Below are the colors currently available. Other colors can be agreed upon separately.

        Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

        18 Available Colors
        Preview colors
        Close

        Colors

        GreenCoat RWS Pro

        Nordic White

        RR1H3 / SS0020

        Regular

        Winter White

        RR20 / SS0005

        Regular

        Snow White

        RR19 / SS0001

        Regular

        Pebble Grey

        RR21 / SS0011

        Regular

        Stone Grey

        RR22 / SS0554

        Regular

        Anthracite Grey

        RR2H8 / SS0087

        Regular

        Mountain Grey

        RR23 / SS0036

        Regular

        Ridge Grey

        RR2F7 / SS0035

        Regular

        Nordic Night Black

        RR33 / SS0015

        Regular

        Walnut Brown

        RR32 / SS0387

        Regular

        Chestnut Brown

        RR887 / SS0435

        Regular

        Acorn Brown

        RR827 / SS0434

        Regular

        Cocoa Brown

        RR8G2 / SS6056

        Regular

        Cottage Red

        RR29 / SS0758

        Regular

        Brick Red

        RR7F2 / SS0742

        Regular

        Pine Green

        RR11 / SS0830

        Regular

        Metallic Silver

        RR40 / SS0045

        Regular

        Metallic Dark Silver

        RR41 / SS0044

        Regular

        The product especially in metallic colors may have slight tonal difference between batches and especially if the time of production differs significantly.

        Reverse Side Coating

        Same coating is applied on both sides of the sheet. Customers can specify the color separately for each side.

        The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

        Reverse side stamping is not applicable for double sided products.