Docol® PHS 1500 press hardening
More about press hardening steelDownload data sheet
Download data sheet
Hardenable boron steel for the automotive industry. Available as both hot rolled and cold rolled. Docol PHS 1500 steels are specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.
Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.
Hot rolled / UC: thickness 2.00-12.00 mm, width up to 1600 mm.
Slit strip and cut to length sheets are available upon request.
Standard | Condition | Test direction |
Typical yield strength Rp0.2 (MPa) |
Typical tensile strength Rm (MPa) | Typical elongation A80 (%) |
Typical elongation A5 (%) |
|
---|---|---|---|---|---|---|---|
Docol PHS FH 1500 | SSAB | Full Hard | T | 960 | 1060 | 4 | — |
Docol PHS CR 1500 | SSAB | As delivered Annealed | T | 340 | 480 | 28 | — |
SSAB | Hot stamped 1) | T | 1200 | 1590 | 6 | — | |
Docol PHS HR 1500 | SSAB | Hot rolled | T | 570 2) | 715 | 20 | 22 |
SSAB | Hot stamped 1) | T | 1200 2) | 1590 | 6 | 7 | |
Docol PHS HR 1500+A | SSAB | Annealed | T | 350 2) | 530 | 25 | 33 |
1) Properties depend on the process.
2) ReH is used instead of Rp0.2.
C (%) |
Si (%) |
Mn (%) |
P (max %) |
S (max %) |
Cr (max %) |
B (%) |
---|---|---|---|---|---|---|
0.20 - 0.25 | 0.15 - 0.35 | 1.00 - 1.35 | 0.025 | 0.005 | 0.35 | 0.0020 - 0.0050 |
Cold rolled (UC): Tolerances in accordance to EN 10131.
Hot rolled (UC): Tolerances in accordance to EN 10051.
Customized dimensional and shape tolerances are available upon request.
Uncoated (UC): available as oiled.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
Заняты разработкой уникальных автомобилестроительных технологий, опробованием новых способов производства или проектированием облегченных конструкционных элементов, способных повысить топливную эффективность, сопротивляемость удару и экологические показатели?
Заказчики имеют круглосуточный доступ к информации о формовке стали Docol®, которая служит для моделирования и выбора прогрессивной высокопрочной стали.