    General Product Description

    The Docol 500LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods. Typical applications include bent profiles. Docol HR500LA-UC can after agreement be adapted and delivered as dual certified with S500MC according to EN 10149-2.

    Dimension Range

    Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

    Slit strip and cut to length sheets are available upon request.

    Grade and coating specific restrictions on available dimensions may occur.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Standard Coating Test direction
      Yield strength Rp0.2
      (MPa)
      Tensile strength Rm
      (MPa)
      Elongation A80 1)
      (min %)
      Elongation A5 2)
      (%)
      Min. inner bending radius for a 90° bend
      Docol HR​500LA VDA 239-100 UC L 500 - 620 560 - 700 14 17 0.8 x t
      Compare parameters

      Select one parameter to compare

      Comparison

        1) A80 value applies for thicknesses < 3.00 mm.

        2) A5 value applies for thicknesses ≥ 3.00 mm.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          Coating C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Al
          (%)
          Ti
          (max %)
          Nb
          (max %)
          Cu
          (max %)
          Docol HR​500LA UC 0.10 0.50 1.60 0.025 0.010 From 0.015 0.15 0.10 0.20
          Compare parameters

          Select one parameter to compare

          Comparison

            Tolerances

            Hot rolled (UC): Tolerances in accordance to EN 10051.

            Customized dimensional and shape tolerances are available upon request.

            Surface Treatments

            Uncoated (UC): available as oiled.

            All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

            Fabrication and Other Recommendations

            For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

            Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

            Docol® High Strength Low Alloy steel product offer

            Docol® 420LA high strength low alloy

            Docol® S600MC high strength low alloy

            Docol® S650MC high strength low alloy

            Docol® S700MC high strength low alloy

            Docol® 460LA high strength low alloy

            Docol® 500LA high strength low alloy

            Docol® 550LA high strength low alloy

            Docol® 600LA high strength low alloy

            Docol® 650LA high strength low alloy

            Docol® 700LA high strength low alloy

            Сопутствующая информация