180

You are currently visiting the SSAB group site

To go to your country specific site please follow this link:

Open sections and profiles from SSAB

Strenx® Section 900

Advanced high-strength, cold-formed steel section

Strenx® Section 900 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 900 MPa.

Its high-strength combined with naturally stiff form enables construction of stronger and lighter structures. Typical applications include demanding load-bearing structures in the lifting, handling and transportation segments.

The steel in Strenx® Section 900 meets or exceeds the requirements of EN 10149-2. Its tolerances meet or exceed, when applicable, the requirements of EN 10162.

Strenx® Section 900 is available as U-section. Other shapes and variations are available upon request.

The maximum length of the sections is 21 meters, cut-to-length sections are available upon request.

Dimension Range

Strenx® Section 900 is available as U-section. Other shapes and variations are available upon request.

   
Bottom length 200 - 400 mm 
Side length 50 - 150mm 
Wall thickness 3.0 - 6.0 mm
Max. length 21 000 mm

Available Standards

EN 10149-2

EN 10162

Strenx® Section 900

Strenx® Section 900

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

DIMENSIONS

T: 3 - 6 mm

L: Up to 21000 mm

STANDARDS

EN 10149-2

EN 10162

DATA SHEET