Strenx® Section 650 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 650 MPa.

Its high-strength combined with naturally stiff form enables construction of stronger and lighter structures. Typical applications include demanding load-bearing structures in the lifting, handling and transportation segments.

The steel in Strenx® Section 650 meets or exceeds the requirements of EN 10149-2. Its tolerances meet or exceed, when applicable, the requirements of EN 10162.

Strenx® Section 650 is available as U-section. Other shapes and variations are available upon request. The maximum length of the sections is 21 meters, cut-to-length sections are available upon request.

Dimension Range

Strenx® Section 650 is available as U-section. Other shapes and variations are available upon request.

   
Bottom length 50 - 400 mm 
Side length 30 - 200 mm 
Wall thickness 2.5 - 10.0 mm
Max. length 21 000 mm

Available Standards

EN 10149-2

EN 10162

EN 1090-2

Strenx® Section 650

Strenx® Section 650

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

DIMENSIONS

T: 2.5 - 10 mm

L: Up to 21000 mm

STANDARDS

EN 10149-2

EN 10162

EN 1090-2

DATA SHEET