180

You are currently visiting the SSAB group site

To go to your country specific site please follow this link:

Open sections and profiles from SSAB
SSAB cold formed lipped C section

Cold-formed lipped C-section

Cold-formed lipped C-section is highly accurate roll formed standard section.

It is manufactured by roll forming using SSAB’s high-quality steels. It is mainly used in the construction, transportation and manufacturing industries where dimensional accuracy and high-quality steels are required. Standard steel grade is S235J2C+N, other steel grades upon request.

Dimension Range (mm)

Available Standards

Lipped C-Sections

Lipped C-Sections

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

DIMENSIONS

STANDARDS

DATA SHEET

English