S235JRH EN 10210

Hollow section for general applications

S235JRH EN10210 is standard hot formed structural hollow section

It is available in circular shape. It is used in engineering and construction.

Dimension Range

S235JRH EN10210 hollow section is available at circular shape. 

   
Circular 26.9 - 133 mm 
Wall thickness 2.0 - 6.30 mm
Mill length 6000 mm

Available Standards

EN 10210-1

EN 10210-2