Mobile crane booms, outriggers and chassis in Strenx® performance steel
10 times the lifting capacity compared to 30 years ago and significantly improved outreach. Mobile crane applications have benefitted enormously from the latest developments in high-strength steel. With its unique and carefully developed chemical composition, Strenx® performance steel makes stronger and tougher welds possible, resulting in safer cranes that lift more and higher.
You can use grades up to Strenx® 1300 MPa to fabricate booms, and Strenx® 960 and Strenx® 1100 for outriggers and chassis.