180
COR TEN A for facades

COR-TEN® A for façades

Cor Ten A for facades

COR-TEN® A is a weathering steel product which can be used in façades without corrosion prevention treatments or paint layers due to its anti-corrosive patina layer on the surface. In order to have a good patina layer, COR-TEN® A needs to be exposed to atmospheric conditions with alternating wet and dry cycles. In addition to excellent corrosion protection, the appearance of a well-formed patina layer is attractive in a natural way. Low maintenance costs, the reduced need for corrosion prevention means less use of paint and solvents, making COR-TEN® A an environmental friendly choice of steel.

More information on how to use COR-TEN® A weathering steel as facade claddings or profiles, can be found in SSAB’s instructions “COR-TEN® Design Guide”.

Dimension Range

Typical COR-TEN® A weathering steel thicknesses for application in façades are 1.0 – 1.5 mm. However, COR-TEN® A weathering steel in cold rolled delivery condition is available in thicknesses ranging from 0.7 – 3.0 mm and widths from 30.0 - 1530 mm as slit coil / coil. Cut to length sheet are available in widths ranging from 1000 – 1530 mm and lengths from 900 mm – 8500 mm. For any further information on dimensions available or special requests, please contact SSAB’s Tech Support at techsupport@ssab.com. 

Appearance

COR-TEN® A weathering steel in cold rolled delivery condition looks like any other cold rolled steel. Typically, it comes with a thin layer of protective oil. As soon as this protective oil is removed, and the steel is exposed to alternating wet & dry atmospheric conditions, the patina layer will start to form.

 

Available Standards

EN 10131

COR-TEN® A for façades

COR-TEN® A for façades

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1530 mm

STANDARDS

EN 10131

DATA SHEET

English