PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1530 mm

STANDARDS

EN 10131

DATA SHEET

English

USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 2 - 12.7 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10051

EN 10029

DATA SHEET

English

PRODUCT NAME
COR-TEN® B
USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 2 - 40 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10051

EN 10029

DATA SHEET

English

PRODUCT NAME
COR-TEN® B-D
USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 2 - 40 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10051

EN 10029

DATA SHEET

English

PRODUCT NAME
COR-TEN B Tube
USED FOR
DIMENSIONS
STANDARDS

EN 10025

EN 1090-2

EN 10219-2

DATA SHEET

English

USED FOR

Structural

Weathering Steel

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1530 mm

STANDARDS

EN 10131

DATA SHEET

English