SSAB Multisteel HS
Normalized or normalized rolled structural steel heavy plate.
SSAB Multisteel HSD and HSE are hot rolled hull structural steel for general marine steel constructions. HS = Hull Structural – D and E = impact strength class. Exceeding the requirements of several classification societies rules, SSAB Multisteel HS is a versatile structural steel for shipbuilding. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.
SSAB Multisteel HS exceeds several steel standards and is available as six societies rules: DNV GL (VL), Lloyd's Register EMEA (LR), American Bureau of Shipping (AB), Bureau Veritas (BV), Registro Italiano Navale (RINA), Russian Maritime Register of Shipping (PC) and also possible to certify to EN10025-2 S355K2+N.
Maximum four (4) different grade if one of them is AB. Otherwise maximum three (3) grades in one plate. Combinations e.g VLD36/ABDH36N/BVDH36/PCD36 or VL D36/BV DH36/S355K2+N.
Please enquiry for suitable combination before placing the order.
CE marking:
SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN10025-1 and EN 10025-2.
The CE marking is marked on an extra page of inspection certification 3.1 for S355K2+N.
CE marking can be given only if S355K2+N is one of the steel grades in the combination.