Product offer and datasheets
SSAB Form product offer

SSAB Form has the versatility you are looking for

SSAB Form comes in a wide range of grades, making it easier for you to optimize your production and the performance of the final product. SSAB Form is delivered as hot rolled strip, cold rolled strip, metal-coated grades, and tubes.
 
Delivered as you like

Delivered as you like it

SSAB Form comes in a wide range of grades, making it easier for you to optimize your production and the performance of the final product. SSAB Form is delivered as hot rolled strip, cold rolled strip, metal-coated grades, and tubes. Delivery condition can be with or without anti-corrosion surface protection.

SSAB Form metal-coated grades for corrosion resistance are available with zinc, galfan, and galvannealed coatings. Zinc coating by hot-dip galvanizing up to 42 μm on both sides can give service life of up to 80 years. Galfan grades give excellent corrosion resistance, weldability, and formability with a thinner 7-23 μm zinc-aluminum coating. Galvannealed grades have a 6-10 μm zinc-iron alloy-coating ideal for spot welding and high-end painting applications.

Many grades to choose from

You can order a wide range of plates, tubes and sections of SSAB Form from our stock network or straight from mill. Smaller volumes are also available to suit your production and storage capacity.

Your local SSAB contact will answer any questions about ordering and shipping, delivery times, marking and packing.


SSAB Form hot rolled products

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Deep Drawing

DIMENSIONS

T: 1.8 - 15 mm

W: Up to 1610 mm

L: Up to 16000 mm

STANDARDS

EN 10051

DATA SHEET

SSAB Form cold rolled products

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Deep Drawing

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10130

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Form 03
USED FOR

Deep Drawing

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10130

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Form 04
USED FOR

Deep Drawing

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10130

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Form 05
USED FOR

Deep Drawing

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10130

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Form 06
USED FOR

Deep Drawing

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10130

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Form 07
USED FOR

Deep Drawing

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

DATA SHEET

SSAB Form tubes

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Form Tube 190
USED FOR
DIMENSIONS
STANDARDS

EN 10305-3

EN 10305-5

DATA SHEET

English

PRODUCT NAME
SSAB Form Tube 220
USED FOR
DIMENSIONS
STANDARDS

EN 10305-3

EN 10305-5

DATA SHEET

English

PRODUCT NAME
SSAB Form Tube 320
USED FOR
DIMENSIONS
STANDARDS

EN 10305-3

EN 10305-5

DATA SHEET

English

PRODUCT NAME
SSAB Form Tube 420
USED FOR
DIMENSIONS
STANDARDS

EN 10305-3

EN 10305-5

DATA SHEET