SSAB Domex product offer
SSAB Domex logo
SSAB Domex logo

HIGH RELIABILITY HIGH VERSATILITY

SSAB Domex® comes as hot rolled plate, hot or cold rolled strip, tubes and sections. It’s also available in different metal-coated grades for corrosion resistance with zinc, galfan and galvannealed coatings.

Hot rolled plate

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex 355ML
USED FOR

Structural

DIMENSIONS

T: 6 - 63 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10029

DATA SHEET
PRODUCT NAME
SSAB Domex 420ML
USED FOR

Structural

DIMENSIONS

T: 7 - 63 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10029

DATA SHEET
PRODUCT NAME
SSAB Domex 460ML
USED FOR

Structural

DIMENSIONS

T: 8 - 63 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10029

DATA SHEET
PRODUCT NAME
SSAB Domex 500ML
USED FOR

Structural

DIMENSIONS

T: 8 - 60 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10029

DATA SHEET

Hot rolled strip

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex 315MC
USED FOR

Structural

DIMENSIONS

T: 1.8 - 18 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10051

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 355MC
USED FOR

Structural

DIMENSIONS

T: 1.8 - 16 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10051

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 420MC
USED FOR

Structural

DIMENSIONS

T: 1.8 - 15 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

EN 10051

DATA SHEET
PRODUCT NAME
SSAB Domex 460MC
USED FOR

Structural

DIMENSIONS

T: 2 - 13 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

EN 10051

DATA SHEET
PRODUCT NAME
SSAB Domex 500MC
USED FOR

Structural

DIMENSIONS

T: 2 - 13 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

EN 10051

DATA SHEET
PRODUCT NAME
SSAB Domex 550MC
USED FOR

Structural

DIMENSIONS

T: 2 - 12.8 mm

W: Up to 1640 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

EN 10051

DATA SHEET
PRODUCT NAME
SSAB Domex 355MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 12 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 420MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 10 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 460MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 4 - 10 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 500MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 8 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET

Cold rolled strip

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex 220LA
USED FOR

Structural

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Domex 260LA
USED FOR

Structural

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 280LA
USED FOR

Structural

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Domex 300LA
USED FOR

Structural

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 340LA
USED FOR

Structural

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 350LA
USED FOR

Structural

DIMENSIONS

T: 0.45 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

DATA SHEET
PRODUCT NAME
SSAB Domex 380LA
USED FOR

Structural

DIMENSIONS

T: 0.4 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 420LA
USED FOR

Structural

DIMENSIONS

T: 0.5 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 460LA
USED FOR

Structural

DIMENSIONS

T: 0.5 - 1.6 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET
PRODUCT NAME
SSAB Domex 500LA
USED FOR

Structural

DIMENSIONS

T: 0.45 - 3 mm

W: Up to 1500 mm

L: Up to 8500 mm

STANDARDS

EN 10131

EN 10268

DATA SHEET

Tubes and sections

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex Tube 460MH
USED FOR
DIMENSIONS
STANDARDS

EN 10219-1

EN 10219-2

DATA SHEET

English

PRODUCT NAME
SSAB Domex Tube 500MH
USED FOR
DIMENSIONS
STANDARDS

EN 10219-2

EN 1090-2

DATA SHEET

English

PRODUCT NAME
SSAB Domex Tube 550MH
USED FOR
DIMENSIONS
STANDARDS

EN 10219-2

EN 1090-2

DATA SHEET

English

USED FOR
DIMENSIONS

T: 2 - 12.5 mm

STANDARDS

EN 10219-1

EN 10219-2

DATA SHEET

English

Metal-coated

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex 220LAD
USED FOR
DIMENSIONS

T: 0.71 - 3 mm

STANDARDS

SSAB

DATA SHEET