180
SSAB Domex Plus
SSAB Domex Plus

New SSAB Domex® Plus speeds up production

SSAB Domex® Plus is part of a new generation of high-strength – low alloy steels (HSLA). The steel adds a new level of performance for stamping, punching, slitting and complicated die forming. SSAB Domex® Plus is particularly well suited to high-volume automated production lines.

Testing of the new Domex® Plus

Take a look how we test the material step by step, and what we evaluate.

Practically burr-free

Thanks to the steel’s fine microstructure the edges show practically no burrs or ridges in mechanical cutting and punching. The cut surface is very smooth and free from micro-cracks, also at very high cutting speeds.

Bend and press without cracks

SSAB Domex® Plus has superior local formability. High-stress bending and forming can be performed without cracks, improving yield and quality of the final product drastically.

The tool-friendly steel

SSAB Domex® Plus has high tolerance for worn tools. When punching tool edges start to become dull and tool clearances are growing, SSAB Domex® Plus keeps performing. Longer production runs and fewer tool changes naturally make the production more cost-effective.
Domex Plus
Daniel Sund

SSAB Domex® Plus

PRODUCT NAME
USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
PRODUCT NAME
SSAB Domex 355MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 12 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 420MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 10 mm

W: Up to 1860 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 460MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 4 - 10 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET
PRODUCT NAME
SSAB Domex 500MC Plus
USED FOR

Structural

Low temperatures (down to -60°)

DIMENSIONS

T: 3 - 8 mm

W: Up to 1800 mm

L: Up to 16000 mm

STANDARDS

EN 10149-2

DATA SHEET

Get in touch

Call or send an email to inquire about prices and how to order SSAB Domex®.

Contact sales