SSAB Boron comes in a wide range of steel grades with carbon contents from 0.22-0.42%. It is available as hot rolled plate; hot rolled coil, slit coil and sheet; cold rolled coil, slit coil and sheet; tubes and sections. Hot rolled strip products are available in black, pickled and annealed condition. Tubes and sections can be produced from hot and cold rolled base material.
In order to suit your production and logistic preferences, SSAB Boron can be sourced directly from our mills or through our stocks. Please consult your local SSAB contact to design the optimal delivery solution for you.
Boron (hardening)
Wear Resistant
T: 0.7 - 80 mm
W: Up to 3300 mm
L: Up to 16000 mm
EN 10131
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 80 mm
W: Up to 3300 mm
L: Up to 16000 mm
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 80 mm
W: Up to 3300 mm
L: Up to 16000 mm
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 1 - 15 mm
W: Up to 3300 mm
L: Up to 16000 mm
EN 10131
EN 10051
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 80 mm
W: Up to 3300 mm
L: Up to 15000 mm
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 16 mm
W: Up to 1800 mm
L: Up to 15000 mm
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 16 mm
W: Up to 1800 mm
L: Up to 16000 mm
EN 10051
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 2 - 15 mm
W: Up to 1800 mm
L: Up to 15000 mm
EN 10051
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 1 - 15 mm
W: Up to 1800 mm
L: Up to 16000 mm
EN 10131
EN 10051
EN 10163-2 Class A, Subclass 3
Boron (hardening)
Wear Resistant
T: 3 - 13 mm
W: Up to 1800 mm
L: Up to 16000 mm
EN 10051
EN 10029
EN 10163-2 Class A, Subclass 3