Hardox® 500 Tuf for tippers
Hardox 500 Tuf for tippers

Hardox® 500 Tuf for tippers

Hardox® 500 Tuf has high strength, extreme hardness and guaranteed toughness in one and the same wear plate. This combination of properties gives tipper bodies superior wear and dent resistance and structural performance.

Typical working conditions for a tipper body made with Hardox® 500 Tuf are the loading and unloading of heavy and sharp rocks in quarries and mines, handling large and heavy steel scrap, and in demolition when pieces of concrete with rebar are loaded or dropped into tippers.
Download "Hardox® 500 Tuf for tippers"

 Ready to upgrade? 

Contact us

Extended service life

Hardox® 500 Tuf can deliver double the service life compared to Hardox® 400 according to calculations with WearCalc and TippCalc for sliding wear with granite.

Tough also in the cold

Hardox® 500 Tuf has high impact toughness even at freezing temperatures. All thicknesses have a guaranteed impact energy of 27 J at -20°C (20 ft-lb at -4°F). For 20 mm plate the typical value is 45 J at -40°C (33 ft-lb at -40°F).

Workshop-friendly

Hardox® 500 Tuf can be processed by the same kind of machinery used for other Hardox® grades. Bendability recommendations are similar to those for Hardox® 450.

Please complete the following information so that we may contact and support you with any Hardox® questions:

By submitting this form, you give SSAB permission to process your personal data, and accept SSAB’s privacy statement. We always follow the local data processing regulations.