In this section, you will find our Nordic quality steels and zinc coatings that we recommend for use with our wide coating offer. Details about product dimensions are also available.
Main applications |
Recommended coating* |
Recommended steels |
Recommended Zinc mass |
Min thickness** |
Usual width range*** |
Roofing, tinsmith
|
Pro BT |
PLX, FAP |
Z350 |
0.60 mm |
1000-1500 mm |
Legacy |
PLX |
Z350 |
0.60 mm |
1000-1500 mm |
|
|
|
|
|
|
Roofing, tiles & profiles |
Pural |
S280GD, S320GD, S350GD
|
Z275 |
0.50 mm |
1000-1500 mm |
Pro BT |
S280GD, S320GD, S350GD
|
Z275 |
0.50 mm |
1000-1500 mm |
Mica BT |
S280GD, S320GD, S350GD
|
Z275 |
0.50 mm |
1000-1500 mm |
Crown BT |
S280GD, S320GD, S350GD
|
Z275 |
0.45 mm |
1000-1500 mm |
Purex |
S280GD, S320GD, S350GD
|
Z275 |
0.45 mm |
1000-1424 mm |
Rough Matt Polyester |
S280GD, S320GD, S350GD
|
Z275 |
0.45 mm |
1000-1424 mm |
Matt Polyester |
S280GD, S320GD, S350GD
|
Z275 |
0.45 mm |
1000-1424 mm |
Polyester |
S280GD, S320GD, S350GD
|
Z275 |
0.42 mm |
1000-1500 mm |
|
|
|
|
|
|
Roofing, modular |
Purex |
S280GD |
Z275 |
0.45 mm |
1000-1424 mm |
|
|
|
|
|
|
Rain water systems |
RWS |
FAX, PLX |
Z275 |
0.50 mm |
1000-1500 mm |
|
|
|
|
|
|
Facade |
Hiarc |
S280GD, S320GD, DX51D
|
Z275 |
0.50 mm |
1000-1500 mm |
Hiarc Max |
S280GD, S320GD, DX51D
|
Z275 |
0.50 mm |
1000-1500 mm |
Hiarc Cool |
S280GD, S320GD, DX51D
|
Z275 |
0.50 mm |
1000-1500 mm |
Anti-Graffiti BT |
S280GD, S320GD, DX51D
|
Z275 |
0.50 mm |
1000-1500 mm |
Crown BT |
S280GD, S320GD, DX51D
|
Z275 |
0.45 mm |
1000-1500 mm |
Polyester |
S280GD, S320GD, DX51D
|
Z275 |
0.42 mm |
1000-1500 mm |
|
|
|
|
|
|
Indoor applications |
Polyester Indoor |
S250GD-S350GD, DX51D
|
Z100 |
0.40 mm |
1000-1424 mm |
Foodsafe BT |
S250GD-S350GD, DX51D
|
Z100 |
0.40 mm |
1000-1500 mm |
Laminate Foodsafe |
S250GD-S350GD, DX51D
|
Z275 |
0.42 mm |
1000-1400 mm |
Epoxy |
S250GD-S350GD, DX51D
|
Z100 |
0.40 mm |
1000-1500 mm |
* Besides these we have a wide range of so called custom made coatings. Please contact SSAB Europe Technical customer support (TCS).
** Please take into account the country specific building recommendations concerning the minimum thickness. And if other thicknesses are required, please contact SSAB technical customer support (TCS). Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Europe Technical customer support (TCS).