180

Just nu besöker du SSAB:s internationella hemsida.

För att besöka den svenska hemsidan, klicka på länken:

GreenCoat Purex

GreenCoat Purex

A modern product with optimized properties for tile profiles and modular roofing

GreenCoat Purex is a durable with an elegant appearance.

GreenCoat Purex possesses excellent forming properties, weather resistance and batch-to-batch color similarity, making it a popular choice for modular roofing. It has greater durability than standard polyester when exposed to people walking on the roof and other roof stresses. A textured finish offers a stylish alternative to roofing sheets and protective flashings.

The reverse side of the sheet is painted as standard with a two-layer grey backside coating. GreenCoat color coated products are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find our Nordic quality steels and zinc coatings that we recommend for use with our wide coating offer. Details about product dimensions are also available.
Learn more

Product details

In this section, you will find our Nordic quality steels and zinc coatings that we recommend for use with our wide coating offer. Details about product dimensions are also available.

Main applications  Recommended coating*  Recommended steels Recommended Zinc mass Min thickness**  Usual width range*** 
Roofing, tinsmith
Pro BT PLX, FAP Z350 0.60 mm 1000-1500 mm
Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles Pural S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
Crown BT S280GD, S320GD, S350GD
Z275 0.45 mm 1000-1500 mm
Purex S280GD, S320GD, S350GD
Z275 0.45 mm 1000-1424 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Matt Polyester S280GD, S320GD, S350GD
Z275 0.45 mm 1000-1424 mm
Polyester S280GD, S320GD, S350GD
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular Purex S280GD Z275 0.45 mm 1000-1424 mm
           
Rain water systems RWS FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facade Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
Hiarc Cool S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm 
Anti-Graffiti BT S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
Crown BT S280GD, S320GD, DX51D 
Z275 0.45 mm 1000-1500 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* Besides these we have a wide range of so called custom made coatings. Please contact SSAB Europe Technical customer support (TCS).
** Please take into account the country specific building recommendations concerning the minimum thickness. And if other thicknesses are required, please contact SSAB technical customer support (TCS). Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Europe Technical customer support (TCS).

Green Coated

GreenCoat Purex

GreenCoat Purex

USED FOR
Main Properties
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Roofing

Main Properties

Outdoor durability

Enhanced formability

Enhanced color and closs repeatability

COATING

Matt

COLOR PALETTE

  • RR1H3 / SS0020 Nordic White

  • RR23 / SS0036 Mountain Grey

  • RR33 / SS0015 Nordic Night Black

  • RR32 / SS0387 Walnut Brown

  • RR887 / SS0435 Chestnut Brown

  • RR29 / SS0758 Cottage Red

  • RR11 / SS0830 Pine Green

DATA SHEET

English