GreenCoat Hiarc Cool
GreenCoar Hiarc Cool

GreenCoat Hiarc Cool

A solar heat reflecting product for facades

GreenCoat Hiarc Cool is the energy efficient product for facades.

GreenCoat Hiarc Cool features special solar heat reflecting pigments that enable surfaces to stay cooler than with regular organic coatings and therefore better air tightness and longer span length in sandwich panels. GreenCoat Hiarc Cool also possesses excellent weathering resistance properties and tolerates forming well. Typical applications include sandwich panels and cladding cassettes. 

The reverse side of the sheet is painted as standard with a two-layer grey backside coating. 

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find our Nordic quality steels and zinc coatings that we recommend for use with our wide coating offer. Details about product dimensions are also available.
Learn more
GreenCoat coils

Thermal Properties

In the table you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties. 
Learn more

In the table below you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties.

Colors  Thermal total solar reflectance1
GreenCoat Hiarc Cool
Standard color  Thermal IR emittance2
GreenCoat Hiarc Cool 
Standard color 
RR23 - Dark Grey  0,265 0,098 0,83 0,87
RR106 - White 0,74 0,74 0,85 0,85
RR40 - Metallic Silver  0,55 0,55 0,68 0,68
RR41 - Metallic Dark Silver  0,38 0,295 0,85 0,72
1) Measurements were taken by an accredited independent test laboratory according to ASTM E903-96
2) Measurements were taken by an accredited independent test laboratory according to ASTM EC1371-98

Standard color

GreenCoat Hiarc Cool

GreenCoat Hiarc Cool

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Facades

MAIN PROPERTIES

Energy efficient

Outdoor durability

COATING

Regular

COLOR PALETTE

  • Frost White
    RR106 / SS0009

  • Mountain Grey
    RR23 / SS0036

  • Metallic Dark Silver
    RR41 / SS0044

DATA SHEET