180
Roofing Natura

Natura

Bio-based coating made with Swedish rapeseed oil (BT)
GreenCoat Pural BT GreenCoat Pural BT GreenCoat Pro BT GreenCoat Pro BT GreenCoat PLX Pro BT GreenCoat PLX Pro BT GreenCoat PLX Pural BT GreenCoat PLX Pural BT GreenCoat Crown BT GreenCoat Crown BT GreenCoat Mica BT
Coating Type
Regular Matt Regular Matt Regular Matt Matt Regular Regular Matt Matt
Corrosion Resistance
RC5 RC5 RC5 RC5 RC5 RC5 RC5 RC5 RC4 RC4 RC5
UV Radiation Resistance
Ruv4 Ruv4 Ruv3 Ruv3 Ruv3 Ruv3 Ruv4 Ruv4 Ruv3 Ruv3 Ruv3
Scratch resistance
40 N 40 N 35 N 35 N 35 N 35 N 40 N 40 N 25 N 25 N 30 N
Minimum inner bending radius
1 x t 1 x t 1.5 x t 1.5 x t 1.5 x t 1.5 x t 1 x sheet thickness*** 1 x sheet thickness 1.5 x t 1.0 x t 1.5 x t
Gloss
40 < 5 40 10 40 10 < 5 40 40 10 5
Stain Resistance
Very good Very good Very good Very good Very good Very good Very good Very good Very good Very good Very good
Coating thickness, nominal
50 µm 50 µm 36 µm 36 µm 36 µm 36 µm 50 µm 50 µm 26 µm 26 µm 30 µm
Fire classification
A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0
Product info Product info Product info Product info Product info Product info Product info Product info Product info Product info Product info