180 180
Roofing
GreenCoat Pro BT

Roofing

Roofs have to deal with Mother Nature´s every mood. Therefore, the material you choose for a roofing product must be able to stand strong against the toughest requirements, look great day after day and offer benefits that can give you cost-savings. 

GreenCoat® products for roofing are characterized by their high quality offering excellent formability, high scratch resistance and long lasting appearance.

GreenCoat® products are UV-resistant (up to RUV4), energy efficient, scratch resistant, have good formability and offer color stability over the years.

In the product function boxes below, we have highlighted our GreenCoat® products in the specific box.

Product offer by product function

- selection by GreenCoat® and general SSAB products

NATURA

Bio-based coating made with Swedish rapeseed oil (BT)


GreenCoat Pural BT
GreenCoat Pro BT
GreenCoat PLX Pro BT
GreenCoat PLX Pural BT
GreenCoat Crown BT
GreenCoat Mica BT

See comparison

Natura

Bio-based coating made with Swedish rapeseed oil (BT)
GreenCoat Pural BT GreenCoat Pural BT GreenCoat Pro BT GreenCoat Pro BT GreenCoat PLX Pro BT GreenCoat PLX Pro BT GreenCoat PLX Pural BT GreenCoat PLX Pural BT GreenCoat Crown BT GreenCoat Crown BT GreenCoat Mica BT
Coating Type
Regular Matt Regular Matt Regular Matt Matt Regular Regular Matt Matt
Corrosion Resistance
RC5 RC5 RC5 RC5 RC5 RC5 RC5 RC5 RC4 RC4 RC5
UV Radiation Resistance
Ruv4 Ruv4 Ruv3 Ruv3 Ruv3 Ruv3 Ruv4 Ruv4 Ruv3 Ruv3 Ruv3
Scratch resistance
40 N 40 N 35 N 35 N 35 N 35 N 40 N 40 N 25 N 25 N 30 N
Minimum inner bending radius
1 x t 1 x t 1.5 x t 1.5 x t 1.5 x t 1.5 x t 1 x sheet thickness*** 1 x sheet thickness 1.5 x t 1.0 x t 1.5 x t
Gloss
40 < 5 40 10 40 10 < 5 40 40 10 5
Stain Resistance
Very good Very good Very good Very good Very good Very good Very good Very good Very good Very good Very good
Coating thickness, nominal
50 µm 50 µm 36 µm 36 µm 36 µm 36 µm 50 µm 50 µm 26 µm 26 µm 30 µm
Fire classification
A1 s1 d0 A1 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A1 s1 d0 A1 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0
Product info Product info Product info Product info Product info Product info Product info Product info Product info Product info Product info

OUTDOOR DURABILITY

Best color and gloss retention over the years


GreenCoat Pural BT
GreenCoat Pro BT
GreenCoat Mica BT
GreenCoat Crown BT

See comparison

OUTDOOR DURABILITY

Best color and gloss retention over the years
GreenCoat Pural BT GreenCoat Pural BT GreenCoat Pro BT GreenCoat Pro BT GreenCoat Mica BT GreenCoat Crown BT GreenCoat Crown BT
Coating Type
Regular Matt Regular Matt Matt Regular Matt
Corrosion Resistance
RC5 RC5 RC5 RC5 RC5 RC4 RC4
UV Radiation Resistance
Ruv4 Ruv4 Ruv3 Ruv3 Ruv3 Ruv3 Ruv3
Scratch resistance
40 N 40 N 35 N 35 N 30 N 25 N 25 N
Minimum inner bending radius
1 x t 1 x t 1.5 x t 1.5 x t 1.5 x t 1.5 x t 1.0 x t
Gloss
40 < 5 40 10 5 40 10
Stain Resistance
Very good Very good Very good Very good Very good Very good Very good
Coating thickness, nominal
50 µm 50 µm 36 µm 36 µm 30 µm 26 µm 26 µm
Fire classification
A1 s1 d0 A1 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0 A2 s1 d0
Product info Product info Product info Product info Product info Product info Product info

COLOR REPEATABILITY

The tightest tolerances for perfect color matches from delivery to delivery


GreenCoat Crown BT

See comparison
GreenCoat Crown BT GreenCoat Crown BT
Coating Type
Regular Matt
Corrosion Resistance
RC4 RC4
UV Radiation Resistance
Ruv3 Ruv3
Scratch resistance
25 N 25 N
Minimum inner bending radius
1.5 x t 1.0 x t
Gloss
40 10
Stain Resistance
Very good Very good
Coating thickness, nominal
26 µm 26 µm
Product info Product info

ENHANCED FORMABILITY

Specialized products for metal roofers/tinsmiths


GreenCoat PLX Pro BT
GreenCoat PLX Pural BT
GreenCoat PLX Legacy

See comparison

ENHANCED FORMABILITY

Specialized products for metal roofers/tinsmiths
GreenCoat PLX Pro BT GreenCoat PLX Pro BT GreenCoat PLX Pural BT GreenCoat PLX Pural BT GreenCoat PLX Legacy
Coating Type
Regular Matt Matt Regular
Corrosion Resistance
RC5 RC5 RC5 RC5
UV Radiation Resistance
Ruv3 Ruv3 Ruv4 Ruv4
Scratch resistance
35 N 35 N 40 N 40 N 15 N
Minimum inner bending radius
1.5 x t 1.5 x t 1 x sheet thickness*** 1 x sheet thickness 2 x t
Gloss
40 10 < 5 40 12
Stain Resistance
Very good Very good Very good Very good
Coating thickness, nominal
36 µm 36 µm 50 µm 50 µm 18 µm
Product info Product info Product info Product info Product info
Natura: These GreenCoat® products use a bio-based coating which uses a substantial portion of Swedish rapeseed oil instead of fossil oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology. The benefits are their proven high quality combined with a durable bio-based coating.
Energy Efficient: GreenCoat Cool provides you with an outer skin on your building that reflects solar radiation. Choose this when you have a building in need of cooling.
Outdoor durability: These GreenCoat® products have our longest guarantees for outdoor durability. They are proven to withstand decades of harsh weather, even in the tough Nordic climate.
Color repeatability: Choose this product when you need special, tight color tolerances for your application. Modular roofing is a typical product application.
Enhanced formability: Products for skilled roofing craftsmen who demand material with high formability. The steels in these products have been developed together with tinsmiths and are formable by hand – even down to -15 °C.