Steel is a superb cladding material. Thanks to its formability, steel provides the designer with truly versatile possibilities to create a surface that matches the environment and the style of the building. Steel is easy and fast to install and maintain, and it has excellent durability.

As an architect, manufacturer or builder, you know that finding a long-lasting color coated material with outstanding environmental properties, high color retention and easy formability can be difficult. This is where GreenCoat® comes into the picture. GreenCoat® products for façades are available in hundreds of colors and finishes, are easy to cut and bend, and stand the test of time.

GreenCoat® products are UV-resistant (up to RUV4), energy efficient, scratch resistant, have good formability and offer color stability over the years.

In the product function boxes below, we have highlighted our GreenCoat® products in the specific box.

Product offer by product function

- selection by GreenCoat® and general SSAB products

NATURA

Bio-based coating made with Swedish rapeseed oil (BT)


GreenCoat Crown BT
GreenCoat Pural Farm BT

 

See comparison

NATURA

Bio-based coating made with Swedish rapeseed oil (BT)
GreenCoat Crown BT GreenCoat Crown BT GreenCoat Pural Farm BT
Coating Type
Regular Matt Regular
Corrosion Resistance
RC4 RC4 RC4
UV Radiation Resistance
Ruv3 Ruv3 Ruv4
Scratch resistance
25 N 25 N 35 N
Minimum inner bending radius
1.5 x t 1.0 x t 1 x t
Gloss
40 10 40
Stain Resistance
Very good Very good Very good
Coating thickness, nominal
26 µm 26 µm 40 µm
Product info Product info Product info

OUTDOOR DURABILITY

Best color and gloss retention over the years


GreenCoat Hiarc
GreenCoat Hiarc Max
GreenCoat Crown BT
GreenCoat Pural Farm BT

See comparison

OUTDOOR DURABILITY

Best color and gloss retention over the years
GreenCoat Hiarc GreenCoat Hiarc GreenCoat Hiarc GreenCoat Hiarc Max GreenCoat Hiarc Max GreenCoat Crown BT GreenCoat Crown BT GreenCoat Pural Farm BT
Coating Type
Regular Matt Shine Effect Regular Matt Regular Matt Regular
Corrosion Resistance
RC4 RC4 RC5 RC5 RC5 RC4 RC4 RC4
UV Radiation Resistance
RUV4 RUV4 RUV4 RUV4 RUV4 Ruv3 Ruv3 Ruv4
Scratch resistance
30N 30N 35N 35N 35N 25 N 25 N 35 N
Minimum inner bending radius
1 x t 1 x t 1 x t 1 x t 1 x t 1.5 x t 1.0 x t 1 x t
Gloss
35*** 4 35 35*** 4 40 10 40
Stain Resistance
Excellent Excellent Excellent Excellent Excellent Very good Very good Very good
Coating thickness, nominal
27 µm**** 27 µm 40 µm 40 µm 40 µm 26 µm 26 µm 40 µm
Product info Product info Product info Product info Product info Product info Product info Product info

COLOR REPEATABILITY

The tightest tolerances for perfect color matches from delivery to delivery


GreenCoat Hiarc
GreenCoat Hiarc Max

See comparison

COLOR REPEATABILITY

The tightest tolerances for perfect color matches from delivery to delivery
GreenCoat Hiarc GreenCoat Hiarc GreenCoat Hiarc GreenCoat Hiarc Max GreenCoat Hiarc Max
Coating Type
Regular Matt Shine Effect Regular Matt
Corrosion Resistance
RC4 RC4 RC5 RC5 RC5
UV Radiation Resistance
RUV4 RUV4 RUV4 RUV4 RUV4
Scratch resistance
30N 30N 35N 35N 35N
Minimum inner bending radius
1 x t 1 x t 1 x t 1 x t 1 x t
Gloss
35*** 4 35 35*** 4
Stain Resistance
Excellent Excellent Excellent Excellent Excellent
Coating thickness, nominal
27 µm**** 27 µm 40 µm 40 µm 40 µm
Fire classification
A1 s1 d0 A1 s1 d0 A1 s1 d0 A1 s1 d0 A1 s1 d0
Product info Product info Product info Product info Product info
Natura: These GreenCoat® products use a bio-based coating which uses a substantial portion of Swedish rapeseed oil instead of fossil oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology. The benefits are their proven high quality combined with a durable bio-based coating.
Outdoor durability: These GreenCoat® products have our longest guarantees for outdoor durability. They are proven to withstand decades of harsh weather, even in the tough Nordic climate.
Color repeatability: Choose these products when you need special, tight color tolerances for your application. Besides the wide color range, these products are offered also in metallic color and special shades.