Dual phase with high formability
Our third generation steels are TRIP assisted dual-phase steels that provide improved formability and good weldability, for ease of use with conventional equipment and lower production costs.
Dual phase with high formability
Metal coated Docol® 600DH-GI and 800DH-GI are two of the steel grades now avaliable and more are on the way.
A special heat treatment producing mainly two-phase structure makes Docol® 600DH-GI and 800DH-GI suitable where an improved formability is requested compared to conventional dual-phase steel grades with the same tensile strength level.
Our Trial Material Stock Center is a unique service to the automotive industry. We ship coils, sheets, and custom lengths of any size to anywhere in the world. In 1-2 weeks the material is ready for dispatch.