Docol® PHS 2000

Docol® PHS 2000 - a new press hardening steel

Hardenable cold rolled boron steel for the automotive industry. Docol® PHS 2000 steels are optimized for parts and components that are manufactured by both direct and indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements. Yield and tensile strengths below are approximate values after press hardening.
Docol® PHS 2000 – a joint development project together with Gestamp

SSAB has launched a new press hardening steel that offers the automotive industry an entirely new level of tensile strength – and a steel optimized for safety components.

Docol® PHS 2000 is the result of a close collaboration between SSAB and automotive component manufacturer Gestamp. The goal of the joint development project was to find an even lighter and cost-effective solution for a bumper component – which it did. Upon project completion, Docol® PHS 2000 helped achieve a 17 percent weight reduction compared to similar bumpers. 
Docol® PHS 2000 maintains crash ductility, while other mechanical properties such as yield strength and ultimate strength have been significantly improved. This means that it is especially useful for components like B-pillars, rockers, bumpers, and BIW structural components requiring high strength and complex geometries. 

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.

Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

*Available upon request.

Available Standards