Docol products for automotive

Docol® 460HE

An automotive steel with improved local formability and hole expansion ratio

The Docol® HE grades are high-strength low-alloy steels with improved local formability. Developed for the most demanding design and production challenges, these automotive steel grades provide improved properties for those facing issues with conventional HSLA material. Typical applications include chassis, seats, mechanisms and powertrains. These grades can also be used for fine blanking. Docol® HE grades meet and exceed EN10149.2. They can be delivered with dual certifications in order to solve current production issues or enable new complex designs without having to change existing standards.

Dimension Range

Docol HR460Y520T HE is available as Hot-rolled pickled and oiled coil, slit coils and cut to length sheets in thickness of 4.00 - 7.00 mm and widths up to 1600 mm. Length up to 16 meters.

Available Standards

SSAB

Docol 460HE

Docol 460HE

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

SSAB

DATA SHEET