Docol products for automotive

Docol 980CP

Cold-rolled, high-strength steels allowing for a tight radius

Docol 980CP is made for cold forming and allows for a tight radius on high-strength applications

These steels are characterized by both a high yield strength and an improved cleanliness, which allows for a tight radius.

We supply many steel grades according to standards like EN, VDA and different OEM standards. If you don't find a specific standard in the table below, please contact your nearest SSAB representative for more detailed information.

Dimension range

Docol CR780Y980T-CP / UC: thickness 0.50-2.10 mm, width up to 1527 mm, length up to 8500 mm.

Docol CR800Y980T-CP / UC: thickness 0.50-2.10 mm, width up to 1527 mm, length up to 8500 mm.

Docol CR780Y980T-CP / GI: thickness 0.80-2.00 mm, width up to 1460 mm, length up to 6000 mm. (upon request)

Slitting to narrow coils and cutting to sheets are available upon request.

Available Standards

VDA 239-100:2016

EN 10131

EN 10143

Docol 980CP

Docol 980CP

USED FOR
STANDARDS
DATA SHEET
USED FOR

Automotive

STANDARDS

VDA239-100:2016

EN 10131

EN 10143

DATA SHEET

English